Cold Work Tool Steel

  • DIN 1.2379 | X155CrVMo12-1 | ASTM D2
  • DIN 1.2080 | X210Cr12 | ASTM D3
  • DIN 1.2436 | X210CrW12 | ASTN D6
  • DIN 1.2510 | 100MnCrW4 | ASTM O1
  • DIN 1.2601 | X165CrMoV12
  • DIN 1.2550 | 60WCrV7
  • DIN 1.2358 | X60CrMoV18-5
  • DIN 1.2360 | 1.2767 | 1.2362 | 1.2842
  • DIN 1.2746 / 45NiCrMoV16-6
  • ASTM/AISI A2 | A8 | S7
  • JIS SKD1 | SKD2 | SKD11 | SKS3 | DC53

Hot Work Tool Steel

  • 1.2344 | H13 | X40CrMoV5-1
  • 1.2343 | H11 | X38CrMoV5-1
  • 1.2581 | H21 | X30WCrV9-3
  • 1.2713 | L6 | 55NiCrMoV6
  • 1.2714 | 6F3 | 56NiCrMoV7
  • 1.2365 | H10 | 32CrMoV12-28
  • DIN 1.2367 | DIN 1.2345 | DIN 86CrMoV7
  • JIS SKD61 | JIS SKD6 | JIS SKD5 | JIS SKT4
  • ASTM/AISI H14 

Plastic Tool Steel

  • 1.2316 | 420H | X36CrMo17
  • DIN 1.2085
  • JIS SUS420J2
  • JIS HMD-1 

High-speed Tool Steel

  • 1.3355 | T1 | S18-0-1
  • 1.3343 | M2 | S6-5-2
  • JIS SKH2 
  • JIS SKH51

Stainless Steel

  • 1.2083 | 420SS | X42Cr13
  • 1.4125 | 440C | X105CrMo17
  • 1.2316 | 420H | X36CrMo17
  • 95Cr18 | 9Cr18Mo
Get Started

Cold Work Tool Steel

  • GB Cr12
  • GB Cr12W
  • GB Cr12MoV 
  • GB Cr12Mo1V1 
  • GB 6CrW2Si 
  • GB 9CrWMn 
  • GB Cr8Mo2SiV
  • GB Cr12V 
  • GB 9SiCr 
  • GB LD 
  • ГОСТ X12 | X12MΦ | 6XB2C | 9XBГ
  • FCS XW-5 | XW-42 | DF-3
  • FCS K100 | K107 | K110 | K460 | K340

Hot Work Tool Steel

  • ГОСТ 4X5MΦ1C
  • ГОСТ 4X5MΦC
  • ГОСТ 3X2B8Φ
  • ГОСТ 5XHM 
  • ГОСТ 3X3M3Φ
  • FCS 8407
  • FCS 8418
  • FCS 2730
  • GB 4Cr5MoSiV1 
  • GB 4Cr5MoSiV
  • GB 3Cr2W8V 
  • GB 5CrNiMo
  • GB 5CrNiMoV 
  • GB 4Cr3Mo3SiV 
  • GB HD
  • FCS W302
  • FCS W300 

Plastic Tool Steel

  • ГОСТ 40X13 
  • FCS S136 
  • FCS S136H 
  • GB 4Cr13 
  • GB 3Cr17NiMo 
  • FCS M310
  • FCS M300

High-speed Tool Steel

  • ГОСТ P18
  • ГОСТ P6M5
  • FCS 2750
  • FCS HSP41
  • GB W18Cr4V
  • GB W6Mo5Cr4V2 
  • FCS S600

Stainless Steel

  • GB 3Cr13 
  • GB 3Cr17 
  • GB 95Cr18
  • GB 2Cr13 
  • GB 9Cr18 
Get Started

Tool Steel In-Stock Inventory

  • 1.2344:Flat Bar & Round Bar
  • 1.2379:Flat Bar & Round Bar
  • D2:Flat Bar & Round Bar
  • H13:Flat Bar & Round Bar
  • SKD11:Flat Bar & Round Bar
  • 1.2316:Flat Bar & Round Bar
  • Follow
  • Follow
  • Follow
  • Follow

Email:[email protected]

Email:[email protected]

24/7 Support: +86-18972782802
  • Home
  • Main Products
  • Tool Steel
  • In-Stock Inventory
  • Contact Us
  • About Us
  • Blogs

P20 Tool Steel Properties & Technical Specifications

by allen | Feb 4, 2026 | plastic tool steel

Introduction: P20 stands as the industry-standard chromium-molybdenum tool steel (AISI P20). You use it specifically for plastic injection molding and die-casting. It comes pre-hardened (28-32 HRC). So, you machine it immediately. This avoids the risk of...
P20 Steel Hardness Guide: From Annealed to Pre-hardened & Re-hardening Tips

P20 Steel Hardness Guide: From Annealed to Pre-hardened & Re-hardening Tips

by allen | Feb 4, 2026 | plastic tool steel

1. Understanding P20 Steel Hardness Levels The right hardness level for P20 steel can make or break your tooling project. Get it wrong, and you’re facing costly failures. It is strictly a trade-off: softer states machine faster but wear out quickly, while harder...
The Ultimate Guide to Customize 1.2316 Steel: Hardness, Dimensions, and Heat Treatment

The Ultimate Guide to Customize 1.2316 Steel: Hardness, Dimensions, and Heat Treatment

by allen | Jan 7, 2026 | plastic tool steel

Picking steel for your tooling isn’t just about checking a grade on a list. It’s about precision engineering that saves you headaches down the line. 1.2316 steel is famous for being the “corrosion killer” in the plastics industry. But here is...
  • Where Is 1.2746 Tool Steel Used? Industries and Tooling Applications
  • Where Is 1.2767 Tool Steel Used? Industries And Molds
  • Why Do 1.2344 Tool Steel Prices Vary? 6 Factors Buyers Should Compare
  • Why Do 1.2344 Tool Steel Prices Vary? 6 Factors Buyers Should Compare
  • How to Choose Tool Steel for Hot Forging Dies
  • 1.2379 | D2 |X155CrVMo12-1
  • 1.2344 | H13 | X40CrMoV5-1
  • 1.2316 | 420H |X36CrMo17
  • D6 | 1.2436 | X210CrW12
  • SKD11
  • SKD61

About

Hubei Fucheng (FCS TOOL STEEL), established in 2007 in Huangshi, China, specializes in producing various tool steels, including cold work tool steel、hot work tool steel、plastic tool steel、high-speed steel and stainless steel. With a monthly output of 2,000 tons, FCS aims to be a leading global supplier, prioritizing quality and customer satisfaction in all its operations.

Main Products

1.2379 | D2 | SKD11 | X155CrVMo12-1

1.2344 | H13 | SKD61 | X40CrMoV5-1

1.2316 | 420H |X36CrMo17

1.2436 | D6 | SKD2 | X210CrW12

1.2083 | 420SS | SUS420J2 | X42Cr13

1.3355 | T1 | SKH2 | S18-0-1

 

Contacts

+86-18972782802

[email protected]

[email protected]

128 Zhangzhihe Avenue, Hekou Town, Xisai District,
Huangshi city, Hubei Province, China

Subscribe

Success!

Subscribe

Stay in touch

  • Follow
  • Follow
  • Follow
Copyright © 2026 all rights reserved
Chat On Whatsapp
Start a Conversation
The team typically replies in a few minutes.
Hi! Click one of our member below to chat on Whatsapp
Wonderful Fucheng Tool Steel
Sales Manager
暂时离线
我们稍后会回复您
抱歉,我们现在不在线。请留下您的消息,我们会尽快回复您。