3Cr17NiMo Tool Steel
3Cr17NiMo integrates the advantages of multiple alloying elements and is strictly produced in accordance with relevant Chinese standards, bringing outstanding performance to the field of plastic mold manufacturing. Through advanced smelting techniques, such as electric arc furnace melting combined with refining technology, the high purity of steel is ensured, laying a solid foundation for its outstanding performance.
3Cr17NiMo Tool Steel – Product Forms & Inventory Specifications
Supply Condition
- Annealed
- Machined
Available Forms
- Round bars
- Plates / Flat bars
- Custom-cut pieces
Processing Services
- Sawing.
- Rough machining.
- Custom heat treatment.
Standard Size Range (Availability varies by stock)
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
3Cr17NiMo Tool Steel – Forming Methods
- Hot Rolled
- Hot Forged
3Cr17NiMo Tool Steel – Surface Finish Options
- Black.
- Grinded.
- Sandblasted.
- Turned/Machined/Milled/Bright.
3Cr17NiMo Tool Steel – Product Forms & Inventory Specifications
Supply Condition
- Annealed
- Machined
Available Forms
- Round bars
- Plates / Flat bars
- Custom-cut pieces
Processing Services
- Sawing.
- Rough machining.
- Custom heat treatment.
Standard Size Range (Availability varies by stock)
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
3Cr17NiMo Tool Steel – Forming Methods
- Hot Rolled
- Hot Forged
3Cr17NiMo Tool Steel – Surface Finish Options
- Black.
- Grinded.
- Sandblasted.
- Turned/Machined/Milled/Bright.
What is 3Cr17NiMo Tool Steel?
3Cr17NiMo (also known as GB/T 3Cr17NiMo, internationally equivalent to DIN 1.2316, AISI 420H) is a kind of martensitic stainless steel specifically used for plastic injection molds, with good corrosion resistance, polishing property and wear resistance. It is suitable for manufacturing mold components with high surface requirements and strong chemical stability.
International Equivalent Grades of 3Cr17NiMo Tool Steel
Chemical Composition of 3Cr17NiMo Tool Steel
3Cr17NiMo Steel Product Specifications

3Cr17NiMo Tool Steel:Typical application fields
It is widely used in the manufacturing of transparent plastics (such as PC, POM, etc.), medical devices, food packaging and electrical grade plastic parts molds, such as:
- Injection molds (with high requirements for surface finish).
- Long-life and highly corrosion-resistant mold bases and cores.
- High mirror finish trim molds, medical plastic parts molds.
- Suitable for use in the food-grade and medical-grade plastic products industry.