40X13 Tool Steel
40X13, also known as 40Cr13 (GB), 4Cr13, is a martensitic stainless tool steel with a medium-high carbon and chromium alloy composition of about 13 per cent. The steel has high hardness, excellent wear resistance and corrosion resistance after tempering treatment, and is suitable for cutting tools and corrosion-resistant parts.
40X13 Tool Steel Size Range
- Hot Rolled Plate/Flat Bar:Thickness: 10-400mm,Width: 200-800mm,Length: 3000-5800mm
- Hot Forged Plate/Flat Bar:Thickness: 50-500mm,Width: 50-1500mm,Length: 3000-5800mm
- Hot Rolled Round Bar: Diameter 10-65mm,Length 3000-5800mm
- Hot Forged Round Bar:Diameter:70-700mm,Length:3000-5800mm
40X13 Tool Steel Surface Finish
Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
40X13 Tool Steel Chemical Composition

40X13 Tool Steel Equivalent Grades

The approximate correspondence of 40X13 in the standards of various countries is as follows:
- Russia (GOST): 40X13 tool steel
- China (GB): 4Cr13 tool steel
- Germany (DIN / W-Nr):X42Cr13/1.2083 tool steel
- Japan (JIS): SUS420J2 tool steel
- USA (AISI/ASTM):420SS tool steel
- Sweden (ASSAB): S136 tool steel
- Austria (BÖHLER): M310 tool steel
40X13 Tool Steel Specifications

40X13 Tool Steel Customized Options

- Custom Surface Conditions: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
- Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
- Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
- Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
- Custom production according to samples or technical agreements.
- 40X13 Tool Steel Electroslag Remelting (ESR): Premium option with higher purity and isotropic properties for critical applications.
40X13 Tool Steel Smelting process

Smelting process: adopting electric furnace or converter melting, strictly controlling the ratio of carbon and chromium, and reducing inclusions through vacuum refining
Heat treatment process:
- Normalising: approx. 840-860 °C, air cooling
- Quenching: about 1020-1050 ℃ oil cooling or air cooling
- Low temperature tempering: 150-250 ℃ for 1-2 times to improve toughness and control cracked areas
Post-treatment: Surface polishing, grinding, nitriding or tempering can be performed to obtain the final dimensions and properties.
40X13 Tool Steel Physical Properties

- Density: 7.75 g/cm³
- Specific heat capacity: 0-100 ℃ about 460 J/kg-K
- Thermal conductivity: 100 ℃ about 28.1 W/m-K; 500 ℃ about 28.9 W/m-K
- Coefficient of linear expansion: 0-100 ℃ about 10.5 × 10-⁶/K; 0-500 ℃ about 12.0 × 10-⁶/K
- Resistivity: ≈0.59 μΩ-m (20 °C)
- Modulus of elasticity: ≈215 GPa (20℃)
40X13 Tool Steel Mechanical & Performance Properties

- Hardness: quenched and tempered to ≥50 HRC (tempered condition hardness).
- Tensile strength: up to 500-955 MPa, yield strength of about 454-595 MPa.
- Impact toughness: tempered state KV about 43 J.
- Corrosion resistance: containing chromium ~ 13% can form a passivation layer, the ability to cope with weak corrosive environment good.
- Wear resistance: medium hardness and high chromium cast into a hard martensitic structure, so that it has good wear resistance.
- Dimensional stability: low distortion after heat treatment and good surface finish.
40X13 Tool Steel Product Applications

-
- Knife manufacturing: kitchen knives, industrial cutting knives, gauges, etc.
- Springs and precision parts: instrument springs, valve discs, compressor parts.
- Corrosive environment parts: parts for moderate corrosion applications in aerospace and chemical equipment.
- Medical devices: some blades and surgical tools.
Additional information