W18Cr4V Tool Steel
W18Cr4V is a tungsten-based high-speed tool steel under the Chinese GB standard, corresponding to AISI T1 / DIN 1.3355. It has excellent wear resistance and red hardness, and is suitable for high-temperature cutting and the manufacturing requirements of high-speed tools.
W18Cr4V Tool Steel – Product Forms & Inventory Specifications
Supply Condition
- Annealed
- Machined
Available Forms
- Round bars
- Plates / Flat bars
- Custom-cut pieces
Processing Services
- Sawing.
- Rough machining.
- Custom heat treatment.
Standard Size Range (Availability varies by stock)
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
W18Cr4V Tool Steel – Forming Methods
- Hot Rolled
- Hot Forged
W18Cr4V Tool Steel – Surface Finish Options
- Black.
- Grinded.
- Sandblasted.
- Turned/Machined/Milled/Bright.
W18Cr4V Tool Steel – Product Forms & Inventory Specifications
Supply Condition
- Annealed
- Machined
Available Forms
- Round bars
- Plates / Flat bars
- Custom-cut pieces
Processing Services
- Sawing.
- Rough machining.
- Custom heat treatment.
Standard Size Range (Availability varies by stock)
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
W18Cr4V Tool Steel – Forming Methods
- Hot Rolled
- Hot Forged
W18Cr4V Tool Steel – Surface Finish Options
- Black.
- Grinded.
- Sandblasted.
- Turned/Machined/Milled/Bright.
What is W18Cr4V Tool Steel?
In modern manufacturing, efficient and precise cutting processing is a key link in ensuring product quality and production efficiency. W18Cr4V high-speed tool steel, as a classic material with outstanding performance, plays an irreplaceable core role in the manufacturing of numerous cutting tools. With its unique chemical composition, excellent physical properties and wide range of applications, it has become one of the preferred materials in industries such as mechanical processing and metal manufacturing.
International Equivalent Grades of W18Cr4V Tool Steel
Chemical Composition of W18Cr4V Tool Steel
W18Cr4V Steel Product Specifications

W18Cr4V Tool Steel:Heat treatment
- Annealing: Hold at approximately 820-860 °C for several hours, then cool slowly to soften to approximately 229-269 HB, providing favorable conditions for subsequent processing.
- Quenching: Preheat to 1270-1280 °C and then cool in oil or air to obtain a high-hardness structure.
- Tempering: It is recommended to temper at least three times (550-570 °C) to ensure uniform structure and stable hardness, ultimately reaching HRC 63-66. It can maintain hardness HRC 62-63 (500-600 °C) even under high temperature cutting.
W18Cr4V Tool Steel:Performance characteristics
- Outstanding red hardness, maintaining cutting sharpness at high temperatures.
- Excellent wear resistance and cutting performance.
- It has good toughness and resistance to brittle cracking, making it suitable for high-load and high-speed cutting.
- The overall stability after processing is high, and it is suitable for batch production tools and precision cutting tools.
Additional information
| Weight | 45 kg |
|---|---|
| Dimensions | 165 × 60 × 25 cm |