1.2367 Tool Steel

At FCS Tool Steel, we offer 1.2367 Tool Steel in multiple supply conditions:

Supply Condition:Annealed,Machined

Available Forms:Round bars,Plates / Flat bars,Custom-cut pieces

Processing Services:Sawing,Rough machining,Custom heat treatment.

Standard Size Range (Availability varies by stock):

  1. Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
  2. Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
  3. Width: 50 – 1000 mm / 50 – 1500 mm.
  4. Forged Discs: Up to Ø1200 mm.

Forming Methods:Hot Rolled,Hot Forged.

Surface Finish Options:Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

1.2367 Tool Steel:Material Introduction

1.2367 Tool Steel:Material Introduction

1.2360 (DIN X38CrMoV5-3) is a high-performance hot work die steel, widely used in high-temperature tool fields such as aluminum alloy die-casting, hot forging, and cooling molds. This steel features excellent hardenability, red hardness and thermal fatigue resistance, and is particularly suitable for environments with complex thermal loads, which can effectively enhance the service life and mold accuracy.

1.2367 Tool Steel:Product Specification

1.2367 Tool Steel:Product Specification

1.2367 Tool Steel:Chemical Composition

1.2367 Tool Steel:Chemical Composition

1.2367 Tool Steel Equivalent Grades

1.2367 Tool Steel Equivalent Grades

1.2367 Tool Steel:Heat treatment suggestions (Reference for Common Process Flows)

1.2360 Tool Steel:Heat treatment suggestions

  1. Annealing (softened state) : Heat to 730-780 °C, furnace cooling ≤ 229 HB
  2. Stress relief: Temper at 600-650 °C for stress release after finishing
  3. Quenching: Heat to 1030-1080 °C → oil cooling/gas cooling, etc
  4. Tempering: 500-550 °C (multiple times) to optimize the balance between toughness and hardness