O1 Tool Steel | 1.2510 |100MnCrW4
As a specialised tool steel supplier, FCS Factory offers O1 (1.2510/100MnCrW4) tool steel, which is a high quality, oil-hardened, cold-worked tool steel with excellent all-round properties. This steel is used in the precision tooling industry where frequent material failure and difficulty in maintaining accuracy are challenges. fcs tool steel O1 provides excellent wear resistance and dimensional stability through optimised alloy design and rigorous production processes, ensuring long life and high accuracy of moulds and tools. Customers have proven that moulds made with FCS TOOL STEEL’s O1 tool steel last 30-50% longer than ordinary materials while maintaining standard dimensional accuracy, significantly reducing production downtime and replacement costs.
O1 Tool Steel | 1.2510 |100MnCrW4 Product Introduction

O1 tool steel (American ASTM Standard)
O1 tool steel is a high carbon, low alloy, oil hardened tool steel (UNS T31501) under the American ASTM standard, with core compositions of carbon (0.85-1.00%), manganese (1.00-1.40%), chromium (0.40-0.60%) and traces of tungsten (0.40-0.60%) and vanadium (≤0.30%). Its properties centre on high dimensional stability and oil hardenability, with a heat-treated hardness of 57-62 HRC, but with moderate wear resistance (industry rating 4/6) and no corrosion resistance due to low chromium content.
1.2510 Tool Steel (German W-Nr/DIN Standard)
1.2510 tool steel is a German W-Nr/DIN numbered cold work tool steel classified as a medium alloy oil hardened steel, the same material as 100MnCrW4. Its composition is based on high carbon (0.90-1.05%), manganese (1.00-1.20%), with the addition of chromium (0.50-0.70%), tungsten (0.50-0.70%) to enhance wear resistance, hardness after quenching up to 60 -65 HRC; properties include low heat distortion (~1% volume change) and high compressive strength (740 N/mm²) with a density of 7.85 g/cm³.
100MnCrW4 tool steel (German DIN material number)
100MnCrW4 tool steel is the equivalent grade of 1.2510 and follows the DIN standard, labelled as a high carbon tungsten-chromium-manganese alloy steel. Its composition is identical to that of 1.2510, but highlights the synergistic strengthening properties of manganese and tungsten: the manganese improves hardenability and the tungsten refines the carbide distribution, resulting in a hardness of 62-65 HRC and a thermal conductivity (30 W/m-K) slightly higher than that of O1 (33 W/m-K).
O1 Tool Steel | 1.2510 |100MnCrW4 Types and Options

The table below shows the size range, surface condition and tolerance details for O1/1.2510/100MnCrW4 Tool Steel:
O1 Tool Steel | 1.2510 |100MnCrW4 Customized Options

- Customized chemical composition: GB, DIN, ASTM, JIS and other standard grades can be produced. Chemical composition can be customized individually.
- Customized specifications: round steel (diameter), plate (thickness, width) can be customized production.
- Specialized packaging for long term storage or extreme transportation conditions: includes spraying black paint all around, wrapping plastic film, spraying anti-rust oil, and shipping in wooden crates.
- Customized production based on samples or technical agreements.
- O1/1.2510/100MnCrW4 Tool Steel Electroslag Remelting (ESR): premium option with higher purity and isotropic properties for critical applications.
O1 Tool Steel | 1.2510 |100MnCrW4 Chemical Composition

O1 Tool Steel | 1.2510 |100MnCrW4 Heat Treatment Process

1.Annealing
2.Quenching
3.Tempering
4.Precautions
Heating process should control the rate of heating to avoid too rapid a rise in temperature leading to workpiece surface oxidation and decarburization. Protective atmosphere heating can be used or placed in the furnace charcoal and other anti-decarburization agent.
When quenching and cooling, choose the appropriate cooling medium and cooling method according to the shape and size of the workpiece to ensure the quenching effect while reducing the risk of deformation and cracking.
O1 Tool Steel | 1.2510 |100MnCrW4 Quality Inspection

1.Surface Condition Inspection
2.Chemical Composition Testing
3.Dimension and Tolerance Inspection
4.Hardness test
5.Ultrasonic Testing
6.Microstructure Inspection
(1) Metallographic Analysis
FCS factory will use metallographic analysis instrument to detect the microstructure state after heat treatment, including carbide distribution, martensite morphology, residual austenite content, etc.
(2) Grain size rating
O1 Tool Steel | 1.2510 |100MnCrW4 Technical Specifications

O1 Tool Steel | 1.2510 |100MnCrW4 Product Applications

Precision Stamping Dies
O1/1.2510/100MnCrW4 tool steel is the ideal material for precision stamping dies due to its excellent wear resistance and dimensional stability. In applications for automotive component manufacturers, precision stamping dies made from our tool steel can handle medium carbon steel plates up to 3mm thick and complete more than one million stamping operations without replacement or reconditioning. They are particularly suitable for stamping processes requiring high surface quality and dimensional accuracy, such as the production of electronic connectors and precision sheet metal parts.
Plastic mould inserts
In plastic injection moulds, O1 tool steel is often used for mould inserts that are subjected to high wear. A supplier of electronic housings uses our tool steel for mould cavity inserts and maintains a mould life of more than 1 million cycles with a dimensional accuracy of ±0.02 mm, even under conditions of reinforced plastic injection moulding with 30% glass fibre. This application is particularly suitable for consumer electronics moulds that require high surface finish and long mould life.
Precision Gauge Manufacturing
1.2510 tool steel excels in gauge manufacturing. A manufacturer of precision measuring instruments uses our tool steel to produce the measuring faces of high-precision calipers and micrometers, which show excellent wear resistance and dimensional stability after heat treatment to 60 HRC. These gauges maintain ±0.001mm measurement accuracy even after prolonged use, meeting the stringent requirements of the aerospace and precision machinery industries.
Woodworking tool applications
In the woodworking industry, 100MnCrW4 tool steel is widely used for planers, milling cutters and carving tools. Woodworking tools made from our tool steel by a high-end furniture manufacturer maintain sharp cutting edges in hardwood machining, significantly reducing downtime due to regrinding and improving productivity and quality. These tools are particularly suited to solid wood furniture and musical instruments that require fine surface finishes.
O1 Tool Steel | 1.2510 |100MnCrW4 Competitive Advantage Comparison

O1 Tool Steel | 1.2510 |100MnCrW4 Customer Success Stories
O1 Tool Steel | 1.2510 |100MnCrW4 Pricing Structure Information
O1 Tool Steel | 1.2510 |100MnCrW4 Frequently Asked Questions

Q:What is the difference between O1, 1.2510 and 100MnCrW4 tool steel?
A: These three standards describe basically the same kind of tool steel, just according to the naming system of different countries or organisations named. O1 tool steel is the American AISI standard, 1.2510 and 100MnCrW4 is the German DIN standard. Their chemical composition and performance characteristics are basically the same, the main difference is that the standards of the composition of the allowable range of subtle differences.Q: What are the advantages over D2 or A2 tool steels?
A: Compared to D2 tool steel, O1 tool steel offers better toughness and lower risk of deformation, but slightly lower wear resistance. Compared to A2, O1 offers better grindability and a higher surface finish that is easier to achieve, but is slightly less resistant to softening at high temperatures.The main advantages of O1 are simplicity of heat treatment, low distortion, good machinability and cost-effectiveness.Q:Can you provide customised sizes?
A:Yes, as a specialised tool steel supplier, we offer flexible delivery options to a wide range of customers. In addition to wholesale service for standard sizes, we also accept customised size requests. For special projects, we offer a cutting service that allows us to supply material to the exact size required by the customer, reducing material waste and processing costs.Q:How do international customers handle imports?
A:First of all, FCS TOOL STEEL has its own tool steel manufacturing plant. In addition, FCS Factory has extensive experience in international trade and can provide comprehensive import and export services to international customers. Our international trade team can assist in the preparation of all necessary import and export documentation. We are familiar with customs requirements in all major markets and can help our clients through the import process. At the same time, we work with a number of international logistics companies to provide competitive shipping solutions.
Additional information
| Weight | 45 kg |
|---|---|
| Dimensions | 165 × 60 × 25 cm |








-1-300x300.png)