Sale!

FCS S136 Tool Steel

FCS supplies its own-brand tool steel; ASSAB S136 is described below for technical comparison only, and the material offered is not original ASSAB S136.

S136 is an electroslag remelting (ESR) pre-hardened stainless plastic mold steel launched by ASSAB, corresponding to international standards such as DIN 1.2083 and AISI 420Mod ESR. It is pre-hardened at the factory (about HB175-215) and can be used without heat treatment. It is particularly suitable for the plastic mold industry that requires anti-corrosion, mirror polishing and high precision.

Tool Steel Size Range

  1. S136 Hot Rolled Plate/Flat Bar:Thickness: 10-400mm,Width: 200-800mm,Length: 3000-5800mm
  2. S136 Hot Forged Plate/Flat Bar:Thickness: 50-500mm,Width: 50-1500mm,Length: 3000-5800mm
  3. S136 Hot Rolled Round Bar: Diameter 10-65mm,Length 3000-5800mm
  4. S136 Hot Forged Round Bar:Diameter:70-700mm,Length:3000-5800mm

Tool Steel Surface Finish

Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

Tool Steel Chemical Composition

Tool Steel Equivalent Grades

S136 Tool Steel Equivalent Grades

The approximate correspondence of S136 in the standards of various countries is as follows:

  1. China (GB): 4Cr13
  2. Germany (DIN / W-Nr):X42Cr13/1.2083
  3. Austria(BOHLER):M310
  4. USA (AISI/ASTM):420SS
  5. Sweden (ASSAB):S136 Tool Steel
  6. Russia (GOST/ГОСТ):40X13
  7. Japan(JIS):SUS420J2

Tool Steel Specifications

Tool Steel Specifications

Tool Steel Customized Options

 Tool Steel Customized Options

  1. Custom Surface Conditions: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
  2. Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
  3. Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
  4. Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
  5. Custom production according to samples or technical agreements.
  6. S136 Tool Steel Electroslag Remelting (S136 ESR): Premium option with higher purity and isotropic properties for critical applications.

Tool Steel Smelting process

Tool Steel Smelting process

Tool Steel Physical Properties

 Tool Steel Physical Properties

  1. Density: approximately 7.85 g/cm³.
  2. Factory hardness: HB 175-215 (pre-hardened state).
  3. Mirror polishing accuracy: Ra can reach ≤0.01 μm.
  4. Heat deformation resistance: Small heat treatment deformation and high dimensional stability.
  5. Corrosion resistance: The high chromium content forms a dense oxide film, making it suitable for humid and corrosive injection molding environments.

Tool Steel Mechanical & Performance Properties

Tool Steel Mechanical & Performance Properties

  1. Outstanding corrosion resistance: Suitable for injection molds of corrosive plastics such as PVC, PMMA, and PC.
  2. Excellent mirror polishing performance: reaching industrial mirror standards (such as optical lens molds).
  3. Wear resistance and moderate hardness: After quenching, it can reach HRC 50-54, durable and maintaining toughness.
  4. Minimal deformation during heat treatment: Suitable for complex-structured molds or large-sized parts.
  5. Good machinability: High processing efficiency in the pre-hardened state, convenient for EDM, boring and milling, and electrical discharge machining.

Tool Steel Product Applications

Tool Steel Product Applications

  1. Precision plastic injection molds (optical lenses, transparent components, medical devices).
  2. Injection molding of corrosive resins such as PVC, POM, and PC.
  3. Medical and food-grade plastic molds.
  4. Small and medium-sized, transparent, optical plastic part molds.
Trademark & Compliance Disclaimer: All brand names, trade names, and registered trademarks mentioned in this publication (such as DC53, 8407, 8418, K110, S136, NAK80, etc.) are the property of their respective trademark holders. References to these grades are provided solely for cross-reference, technical comparison, and identification purposes, and do not imply any affiliation with, endorsement by, or direct sale of products from the original trademark owners.

Additional information

Weight 45 kg
Dimensions 165 × 60 × 25 cm