S600 Tool Steel
S600 Tool Steel corresponds to grades such as 1.3343 ,S6-5-2, M2 ,SKH51 ,HSP41 ,W6Mo5Cr4V2 ,P6M5, etc. in multiple global standards.
Supply status and size specifications of S600
- S600 Delivery condition: Annealed state (HB ≤248)
- S600 Supply forms: round steel, flat steel, plates, forgings, custom cutting
- S600 Optional sizes: Diameter Φ10 ~ Φ65/Φ 70 ~ Φ400/500/600/700 mm,thickness 8-45/50-500mm,width 50-1000mm/50-1500mm, Forged disc ≤ 1200mm,
etc
S600 Tool Steel Forming Process Options
S600 Hot Rolled,S600 Hot Forged
S600 Tool Steel Surface Finish
Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
What is S600 tool steel?
BOHLER/Böhler S600 (1.3343 / S6-5-2 /ASTM M2 / SKH51) is a typical high-speed tool steel with high thermal hardness, high wear resistance and good toughness. It features high grinding performance and thermal stability, making it suitable for a wide range of high-speed cutting, stamping, mold and wear-resistant component manufacturing. Due to its superior performance, compliance with multiple international standards and wide application.
What are the specifications of S600 tool steel?

What are the Equivalent Grades of S600 Tool Steel?
What is the Chemical Composition of S600 Tool Steel?
What are the Customized Options of S600 Tool Steel ?
- Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
- Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
- Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
- Custom production according to samples or technical agreements.
- S600 Tool Steel Electroslag Remelting (S600 ESR): Premium option with higher purity and isotropic properties for critical applications.
What is the Smelting process of S600 Tool Steel ?

S600 Tool Steel Physical properties
- Toughness and ductility: High
- Wear resistance: High
- Compressive strength: High
- Edge stability: High
- Grinding property: High
- Red hardness (thermal hardness) : High
In practical applications, the common density of typical M2 is approximately 8.12 kg/dm³, the elastic modulus is about 224 GPa, and the coefficient of thermal expansion is approximately 10.5×10⁻⁶/K (refer to data similar to 1.3343).
S600 Tool Steel Typical application fields

- Steel milling cutters, screw drills, taps, broaches, and precision blanking die tools.
- Cold stamping, drawing, powder pressing tools, standard parts (pins, punches).
- Gear cutting, shaving tools, plastic injection systems, automotive parts (turbines, sensors).
- Food industry blades, shears, hobs, shearing machine tools, wear-resistant parts, etc.
Additional information
| Weight | 45 kg |
|---|---|
| Dimensions | 180 × 40 × 30 cm |