W302 Tool Steel

W302 Tool Steel corresponds to grades such as 1.2344,H13,SKD61,4Cr5MoSiV1,4X5MΦ1C,X40CrMoV5-1,8407, etc. in multiple global standards.

Supply status and size specifications of W302

  1. W302 Delivery condition: Annealed state (HB ≤255)
  2. W302 Supply forms: round steel, flat steel, plates, forgings, custom cutting
  3. W302 Optional sizes: Diameter Φ10 ~ Φ65/Φ 70 ~ Φ400/500/600/700 mm,thickness 8-45/50-500mm,width 50-1000mm/50-1500mm, Forged disc ≤ 1200mm,
    etc

W302 Tool Steel Forming Process Options

W302 Hot Rolled,W302 Hot Forged

K302 Tool Steel Surface Finish

Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

What is W302 tool steel?

Austrian (Böhler) W302 (also known as H13 hot work tool steel) is a hot work tool steel containing approximately 5% chromium, specifically designed for applications that are subject to thermal shock, friction, and high stress in high-temperature environments. If one wants to further enhance the purity and uniformity of the structure, electroslag remelting (ESR) can be adopted.

What are the specifications of W302 tool steel?

Specifications : W302 tool steel

What are the Equivalent Grades of W302 Tool Steel?

the Equivalent Grades of W302 Tool Steel

What is the Chemical Composition of W302 Tool Steel?

the Chemical Composition of W302 Tool Steel

What are the Customized Options of W302 Tool Steel ?

  1. Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
  2. Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
  3. Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
  4. Custom production according to samples or technical agreements.
  5. W302 Tool Steel Electroslag Remelting (W302 ESR): Premium option with higher purity and isotropic properties for critical applications.

What is the Smelting process of W302 Tool Steel ?

Tool Steel Smelting process:W302

W302 Tool Steel Physical properties

  1. Density approximately 0.282 lb/in³ (≈7.80 g/cm³).
  2. Elastic modulus: approximately 165  gp@room temperature; It drops to ~176  gp@500  °C with temperature rise.
  3. Coefficient of linear expansion: 11.5-13.2 µm/m·°C, slightly increasing with rising temperature.
  4. Both thermal conductivity and resistivity perform well, and it has both heat resistance and thermal conductivity.

W302 Tool Steel Typical application fields

Tool Steel Product Applications

W302 is widely used in the following high-temperature tools and components:

  1. Hot working dies: including forging dies, extrusion dies, and low/high-pressure casting dies.
  2. Injection and blow molding industry molds: thermoplastic molding, hot runner system components.
  3. Hot stamping and hot forging processing tools: shearing knives, die cores, etc. for heat-resistant shock conditions.
  4. Mechanical and automotive parts: such as die-casting templates, nuts, heat treatment fixtures, etc.