Sale!

K460 Tool Steel

K460 Tool Steel corresponds to grades such as 1.2510,O1,SKS3,9CrWMn,100MnCrW4,9XBГ,DF-3, etc. in multiple global standards.

Supply status and size specifications of K460

  1. K460 Delivery condition: Annealed state (HB ≤ 230)
  2. K460 Supply forms: round steel, flat steel, plates, forgings, custom cutting
  3. K460 Optional sizes: Diameter Φ10 ~ Φ65/Φ 70 ~ Φ400/500/600/700 mm,thickness 8-45/50-500mm,width 50-1000mm/50-1500mm, Forged disc ≤ 1200mm,
    etc

K460 Tool Steel Forming Process Options

K460 Hot Rolled,K460 Hot Forged

K460 Tool Steel Surface Finish

Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

What is K460 tool steel?

Böhler K460 is a cold work tool steel with high carbon, medium chromium and tungsten (corresponding to German grade 1.2510, equivalent to EN/DIN 100MnCrW4 / ASTM O1). It incorporates tungsten into its structure to enhance its resistance to abrasive wear while maintaining excellent toughness and low deformation quenching characteristics. Its heat treatment process is simple: low-temperature quenching followed by one tempering is sufficient, making it suitable for cost-sensitive applications where moderate wear resistance is required.

What are the specifications of K460 tool steel?

Specifications : K460 tool steel

What are the Equivalent Grades of K460 Tool Steel?

the Equivalent Grades of K460 Tool Steel

What is the Chemical Composition of K460 Tool Steel?

the Chemical Composition of K460 Tool Steel

What are the Customized Options of K460 Tool Steel ?

  1. Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
  2. Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
  3. Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
  4. Custom production according to samples or technical agreements.
  5. K460 Tool Steel Electroslag Remelting (K460 ESR): Premium option with higher purity and isotropic properties for critical applications.

What is the Smelting process of K460 Tool Steel ?

Tool Steel Smelting process:K460

K460 Tool Steel Physical properties

  1. Toughness and ductility: High
  2. Wear resistance: Good
  3. Compressive strength: Extremely high
  4. Dimensional stability: Good
  5. Grinding performance: High

K460 Tool Steel Typical application fields

Tool Steel Product Applications

K460 steel is widely used in the following fields:

  1. Stamping and shearing tools: fine punching, punching, trimming, etc.
  2. Plastic molds: used for cold heading parts that require good grindability and stability.
  3. Thread cutting tools: Suitable for fine and precise cutting.
  4. Industrial cutting tools: Machine tool inserts and shearing tools for the papermaking, wood, and recycling industries.

Additional information

Weight 45 kg
Dimensions 180 × 40 × 30 cm