1.2379 Tool Steel Stock:Flat Bar & Round Bar
1.2379 Tool Steel Clearance Hot Sale | Abundant Stock, Same-Day Shipment!
1.2379 cold work die steel is in stock clearance. Round bars (turned round bars, peeled round bars) and black surface plates (black surface plates, milled surface plates) with various specifications are available. Custom cutting as needed is supported, with in-stock items shipped quickly. Quantities are limited. It is suitable for high-wear-resistance die applications such as blanking dies and cold extrusion dies. Welcome to order now!
1.2379 Flat Bar-Turned
FCS Tool Steel Manufacturer Stocklist(2025.07.31) |
|||||||||
Stock No. |
Grade |
Shape |
Surface |
Process |
Thickness/Diameter |
Width |
Length |
PCS |
Weight(KG) |
| FC000008566 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 50 | 600 | 3540 | 1 | 852 |
| FC000008567 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 50 | 600 | 3720 | 1 | 904 |
| FC000008568 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 50 | 600 | 3620 | 1 | 880 |
| FC000005043 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 56 | 610 | 2637.1 | 1 | 736 |
| FC000005052 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 60 | 610 | 2930 | 1 | 838 |
| FC000008569 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 65 | 600 | 2820 | 1 | 884 |
| FC000008570 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 65 | 600 | 2950 | 1 | 910 |
| FC000000649 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 70 | 370 | 3168.6 | 1 | 668 |
| FC000008565 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 80 | 600 | 2940 | 1 | 1132 |
| FC000000632 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 510 | 4048.7 | 1 | 1500 |
| FC000000633 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 510 | 2901.6 | 1 | 1075 |
| FC000000634 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 510 | 2893.5 | 1 | 1072 |
| FC000000667 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 510 | 4091.9 | 1 | 1516 |
| FC000007092 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 500 | 2879.4 | 1 | 1046 |
| FC000008197 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 605 | 3397.9 | 1 | 1492 |
| FC000008571 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 90 | 600 | 3435 | 1 | 1446 |
| FC000007094 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 95 | 405 | 2478.5 | 1 | 770 |
| FC000007095 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 95 | 405 | 2942 | 1 | 914 |
| FC000000638 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 100 | 510 | 3237.9 | 1 | 1330 |
| FC000000640 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 100 | 510 | 2220.3 | 1 | 912 |
| FC000009188 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 100 | 610 | 3265 | 1 | 1554 |
| FC000009189 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 100 | 610 | 3210 | 1 | 1520 |
| FC000007933 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 110 | 610 | 2920 | 1 | 1518 |
| FC000000655 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 120 | 605 | 3513.8 | 1 | 2046 |
| FC000000665 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 120 | 505 | 3856 | 1 | 1876 |
| FC000009186 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 120 | 610 | 3355 | 1 | 1910 |
| FC000009187 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 120 | 610 | 3410 | 1 | 1958 |
| FC000006547 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 125 | 610 | 3580.3 | 1 | 2188 |
| FC000007932 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 125 | 610 | 3940 | 1 | 2348 |
| FC000000656 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 127 | 610 | 3737.4 | 1 | 2320 |
| FC000000657 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 127 | 610 | 3212.2 | 1 | 1994 |
| FC000000651 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 130 | 610 | 3415 | 1 | 2120 |
| FC000008199 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 130 | 605 | 3476.1 | 1 | 2190 |
| FC000006868 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 140 | 610 | 4144.5 | 1 | 2832 |
| FC000007091 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 140 | 610 | 2180.6 | 1 | 1490 |
| FC000000652 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 150 | 610 | 3315 | 1 | 2336 |
| FC000007934 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 150 | 610 | 2580 | 1 | 1852 |
| FC000001800 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 180 | 610 | 3685 | 1 | 3186 |
| FC000001801 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 180 | 610 | 3505 | 1 | 3052 |
| FC000000663 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 200 | 610 | 3973.1 | 1 | 3862 |
| FC000000635 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 202 | 208 | 2120 | 1 | 870 |
| FC000007087 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 230 | 230 | 2931.6 | 1 | 1244 |
| FC000007088 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 240 | 240 | 2837.8 | 1 | 1310 |
| FC000007093 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 242 | 252 | 3451.9 | 1 | 1686 |
| FC000008193 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 270 | 610 | 3345 | 1 | 4250 |
| FC000000647 | 1.2379 | Flat Bar | Turned | EF+LF+VD | 292 | 302 | 3121.1 | 1 | 2197 |
1.2379 Flat Bar-Black
FCS Tool Steel Manufacturer Stocklist(2025.07.31) |
|||||||||
Stock No. |
Grade |
Shape |
Surface |
Process |
Thickness/Dia |
Width |
Length |
PCS |
Weight(KG) |
| FC000000307 | 1.2379 | Flat Bar | Black | EF+LF+VD | 40 | 180 | 2901.6 | 1 | 164 |
| FC000000308 | 1.2379 | Flat Bar | Black | EF+LF+VD | 50 | 200 | 2624.2 | 1 | 206 |
| FC000000309 | 1.2379 | Flat Bar | Black | EF+LF+VD | 50 | 200 | 2980.9 | 1 | 234 |
| FC000000310 | 1.2379 | Flat Bar | Black | EF+LF+VD | 50 | 200 | 3082.8 | 1 | 242 |
| FC000000311 | 1.2379 | Flat Bar | Black | EF+LF+VD | 50 | 240 | 3078.6 | 1 | 290 |
| FC000000316 | 1.2379 | Flat Bar | Black | EF+LF+VD | 50 | 250 | 2690.4 | 1 | 264 |
| FC000000314 | 1.2379 | Flat Bar | Black | EF+LF+VD | 60 | 280 | 2608.4 | 1 | 344 |
| FC000001290 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 105 | 4031.6 | 1 | 216 |
| FC000001291 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 105 | 4106.3 | 1 | 220 |
| FC000001292 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 105 | 4181 | 1 | 224 |
| FC000001294 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 155 | 3540.3 | 1 | 280 |
| FC000001295 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 105 | 4292.9 | 1 | 230 |
| FC000001297 | 1.2379 | Flat Bar | Black | EF+LF+VD | 65 | 105 | 3135.7 | 1 | 168 |
| FC000000315 | 1.2379 | Flat Bar | Black | EF+LF+VD | 70 | 260 | 2617.8 | 1 | 374 |
| FC000001289 | 1.2379 | Flat Bar | Black | EF+LF+VD | 80 | 155 | 4571.6 | 1 | 445 |
| FC000001293 | 1.2379 | Flat Bar | Black | EF+LF+VD | 80 | 130 | 3233.7 | 1 | 264 |
| FC000001298 | 1.2379 | Flat Bar | Black | EF+LF+VD | 80 | 80 | 1950.6 | 1 | 98 |
| FC000001299 | 1.2379 | Flat Bar | Black | EF+LF+VD | 80 | 80 | 4518.3 | 4 | 908 |
| FC000001296 | 1.2379 | Flat Bar | Black | EF+LF+VD | 205 | 205 | 2655.4 | 1 | 876 |
1.2379 Round Bar-Turned
FCS Tool Steel Manufacturer Stocklist(2025.07.31) |
||||||||
Stock No. |
Grade |
Shape |
Surface |
Process |
Thickness/Diameter |
Length |
PCS |
Weight(KG) |
| FC000008991 | 1.2379 | Round Bar | Turned | EF+LF+VD | 61 | 4369.6 | 22 | 2280 |
| FC000002610 | 1.2379 | Round Bar | Turned | EF+LF+VD | 70 | 3215.1 | 1 | 100 |
| FC000006291 | 1.2379 | Round Bar | Turned | EF+LF+VD | 70 | 3443.1 | 11 | 1178 |
| FC000006296 | 1.2379 | Round Bar | Turned | EF+LF+VD | 70 | 2577.5 | 12 | 962 |
| FC000008992 | 1.2379 | Round Bar | Turned | EF+LF+VD | 71 | 3839.3 | 5 | 614 |
| FC000002599 | 1.2379 | Round Bar | Turned | EF+LF+VD | 90 | 3787.2 | 4 | 774 |
| FC000002603 | 1.2379 | Round Bar | Turned | EF+LF+VD | 90 | 2922.7 | 3 | 448 |
| FC000002710 | 1.2379 | Round Bar | Turned | EF+LF+VD | 90 | 2348.6 | 1 | 120 |
| FC000006293 | 1.2379 | Round Bar | Turned | EF+LF+VD | 90 | 3314.2 | 6 | 1016 |
| FC000004869 | 1.2379 | Round Bar | Turned | EF+LF+VD | 100 | 2478.5 | 1 | 156 |
| FC000004870 | 1.2379 | Round Bar | Turned | EF+LF+VD | 100 | 2415 | 1 | 152 |
| FC000004872 | 1.2379 | Round Bar | Turned | EF+LF+VD | 100 | 2224.3 | 1 | 140 |
| FC000006923 | 1.2379 | Round Bar | Turned | EF+LF+VD | 100 | 2069 | 9 | 1172 |
| FC000002562 | 1.2379 | Round Bar | Turned | EF+LF+VD | 110 | 3499.1 | 1 | 266 |
| FC000002563 | 1.2379 | Round Bar | Turned | EF+LF+VD | 110 | 3025.5 | 1 | 230 |
| FC000002613 | 1.2379 | Round Bar | Turned | EF+LF+VD | 110 | 1631.1 | 1 | 124 |
| FC000004864 | 1.2379 | Round Bar | Turned | EF+LF+VD | 110 | 4183.1 | 1 | 318 |
| FC000002555 | 1.2379 | Round Bar | Turned | EF+LF+VD | 120 | 4317.3 | 1 | 390 |
| FC000002556 | 1.2379 | Round Bar | Turned | EF+LF+VD | 120 | 2811.8 | 1 | 254 |
| FC000002557 | 1.2379 | Round Bar | Turned | EF+LF+VD | 120 | 2523.9 | 1 | 228 |
| FC000002596 | 1.2379 | Round Bar | Turned | EF+LF+VD | 120 | 2435.4 | 1 | 220 |
| FC000005472 | 1.2379 | Round Bar | Turned | EF+LF+VD | 120 | 5147 | 1 | 465 |
| FC000008327 | 1.2379 | Round Bar | Turned | EF+LF+VD | 121 | 2285 | 1 | 204 |
| FC000007985 | 1.2379 | Round Bar | Turned | EF+LF+VD | 122 | 5325 | 1 | 492 |
| FC000007986 | 1.2379 | Round Bar | Turned | EF+LF+VD | 122 | 5210 | 1 | 480 |
| FC000007987 | 1.2379 | Round Bar | Turned | EF+LF+VD | 122 | 5260 | 1 | 484 |
| FC000002558 | 1.2379 | Round Bar | Turned | EF+LF+VD | 130 | 2172.2 | 1 | 230 |
| FC000002559 | 1.2379 | Round Bar | Turned | EF+LF+VD | 130 | 2795.5 | 1 | 296 |
| FC000002612 | 1.2379 | Round Bar | Turned | EF+LF+VD | 130 | 2134.4 | 1 | 226 |
| FC000004998 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4495 | 1 | 468 |
| FC000004999 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4615 | 1 | 480 |
| FC000005000 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4545 | 1 | 474 |
| FC000005001 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4470 | 1 | 466 |
| FC000005443 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4455 | 1 | 466 |
| FC000005444 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 3620 | 1 | 380 |
| FC000005446 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4345 | 1 | 454 |
| FC000005447 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4350 | 1 | 454 |
| FC000005448 | 1.2379 | Round Bar | Turned | EF+LF+VD | 131 | 4155 | 1 | 434 |
| FC000002592 | 1.2379 | Round Bar | Turned | EF+LF+VD | 135 | 2874.2 | 1 | 328 |
| FC000002509 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4337 | 1 | 532 |
| FC000002510 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4516.3 | 1 | 554 |
| FC000002511 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3831.5 | 1 | 470 |
| FC000002512 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3913.1 | 1 | 480 |
| FC000002513 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3864.2 | 1 | 474 |
| FC000002515 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3880.5 | 1 | 476 |
| FC000002516 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4141.3 | 1 | 508 |
| FC000002517 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4173.9 | 1 | 512 |
| FC000002518 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4353.3 | 1 | 534 |
| FC000002519 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3815.2 | 1 | 468 |
| FC000002520 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3978.3 | 1 | 488 |
| FC000002521 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4972.9 | 1 | 610 |
| FC000002522 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4434.8 | 1 | 544 |
| FC000002523 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4271.8 | 1 | 524 |
| FC000002527 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4010.9 | 1 | 492 |
| FC000002537 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2478.3 | 1 | 304 |
| FC000002538 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3293.5 | 1 | 404 |
| FC000002539 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3456.5 | 1 | 424 |
| FC000002540 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2641.3 | 1 | 324 |
| FC000002541 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4353.3 | 1 | 534 |
| FC000002542 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4076.1 | 1 | 500 |
| FC000002543 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2722.8 | 1 | 334 |
| FC000002544 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3293.5 | 1 | 404 |
| FC000002545 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 4434.8 | 1 | 544 |
| FC000002546 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3032.6 | 1 | 372 |
| FC000002547 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3815.2 | 1 | 468 |
| FC000002548 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2722.8 | 1 | 334 |
| FC000002550 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3798.9 | 1 | 466 |
| FC000002552 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3146.8 | 1 | 386 |
| FC000002587 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2869.6 | 1 | 352 |
| FC000002588 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2706.5 | 1 | 332 |
| FC000002589 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 2706.5 | 1 | 332 |
| FC000002590 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 3782.6 | 1 | 464 |
| FC000004865 | 1.2379 | Round Bar | Turned | EF+LF+VD | 140 | 5021.8 | 1 | 616 |
| FC000003717 | 1.2379 | Round Bar | Turned | EF+LF+VD | 141 | 3584.9 | 1 | 446 |
| FC000001253 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 4465 | 1 | 548 |
| FC000001254 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 4560 | 1 | 560 |
| FC000001255 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 4600 | 1 | 568 |
| FC000001259 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 3375 | 1 | 416 |
| FC000001260 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 4425 | 1 | 546 |
| FC000001265 | 1.2379 | Round Bar | Turned | EF+LF+VD | 142 | 3820 | 1 | 472 |
| FC000002553 | 1.2379 | Round Bar | Turned | EF+LF+VD | 145 | 2722 | 1 | 358 |
| FC000002554 | 1.2379 | Round Bar | Turned | EF+LF+VD | 145 | 2752.4 | 1 | 362 |
| FC000001791 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 3180 | 1 | 450 |
| FC000002490 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4475 | 1 | 632 |
| FC000002491 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4279.1 | 1 | 602 |
| FC000002492 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4280 | 1 | 604 |
| FC000002493 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 3985 | 1 | 560 |
| FC000002495 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4360 | 1 | 616 |
| FC000002497 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4505 | 1 | 630 |
| FC000002498 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4392.9 | 1 | 618 |
| FC000002499 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4315 | 1 | 610 |
| FC000002502 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4392.9 | 1 | 618 |
| FC000002503 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4137 | 1 | 582 |
| FC000002504 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4364.4 | 1 | 614 |
| FC000002505 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4407.1 | 1 | 620 |
| FC000002506 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4364.4 | 1 | 614 |
| FC000002507 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4506.6 | 1 | 634 |
| FC000002508 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 4506.6 | 1 | 634 |
| FC000002531 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2416.8 | 1 | 340 |
| FC000002532 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2104 | 1 | 296 |
| FC000002534 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2560 | 1 | 360 |
| FC000002535 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2999.7 | 1 | 422 |
| FC000002536 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 1691.8 | 1 | 238 |
| FC000002564 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2772.2 | 1 | 390 |
| FC000008322 | 1.2379 | Round Bar | Turned | EF+LF+VD | 150 | 2725 | 1 | 394 |
| FC000001251 | 1.2379 | Round Bar | Turned | EF+LF+VD | 151 | 4215 | 1 | 600 |
| FC000001252 | 1.2379 | Round Bar | Turned | EF+LF+VD | 151 | 4230 | 1 | 602 |
| FC000008328 | 1.2379 | Round Bar | Turned | EF+LF+VD | 152 | 4570 | 1 | 652 |
| FC000008054 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4750 | 1 | 768 |
| FC000008055 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4855 | 1 | 788 |
| FC000008056 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4865 | 1 | 788 |
| FC000008057 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4885 | 1 | 788 |
| FC000008058 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4935 | 1 | 796 |
| FC000008059 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4110 | 1 | 664 |
| FC000008060 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 5000 | 1 | 808 |
| FC000008061 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 5080 | 1 | 822 |
| FC000008064 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 4830 | 1 | 778 |
| FC000008241 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 1960 | 1 | 318 |
| FC000008242 | 1.2379 | Round Bar | Turned | EF+LF+VD | 162 | 3070 | 1 | 496 |
| FC000008062 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4820 | 1 | 876 |
| FC000008063 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4910 | 1 | 894 |
| FC000008065 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4820 | 1 | 876 |
| FC000008066 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4925 | 1 | 900 |
| FC000008067 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4695 | 1 | 856 |
| FC000008068 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4930 | 1 | 896 |
| FC000008243 | 1.2379 | Round Bar | Turned | EF+LF+VD | 172 | 4780 | 1 | 870 |
| FC000003301 | 1.2379 | Round Bar | Turned | EF+LF+VD | 175 | 4164.9 | 1 | 796 |
| FC000006213 | 1.2379 | Round Bar | Turned | EF+LF+VD | 180 | 5700 | 1 | 1132 |
| FC000006214 | 1.2379 | Round Bar | Turned | EF+LF+VD | 180 | 5695 | 1 | 1132 |
| FC000007595 | 1.2379 | Round Bar | Turned | EF+LF+VD | 180 | 4551.4 | 1 | 920 |
| FC000008320 | 1.2379 | Round Bar | Turned | EF+LF+VD | 180 | 2060 | 1 | 424 |
| FC000008321 | 1.2379 | Round Bar | Turned | EF+LF+VD | 180 | 2530 | 1 | 522 |
| FC000004928 | 1.2379 | Round Bar | Turned | EF+LF+VD | 182 | 5635 | 1 | 1136 |
| FC000004934 | 1.2379 | Round Bar | Turned | EF+LF+VD | 182 | 5635 | 1 | 1130 |
| FC000005106 | 1.2379 | Round Bar | Turned | EF+LF+VD | 182 | 5180 | 1 | 1040 |
| FC000005107 | 1.2379 | Round Bar | Turned | EF+LF+VD | 182 | 3790 | 1 | 762 |
| FC000006210 | 1.2379 | Round Bar | Turned | EF+LF+VD | 190 | 5085 | 1 | 1124 |
| FC000006211 | 1.2379 | Round Bar | Turned | EF+LF+VD | 190 | 5045 | 1 | 1118 |
| FC000006212 | 1.2379 | Round Bar | Turned | EF+LF+VD | 190 | 4755 | 1 | 1054 |
| FC000001792 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4620 | 1 | 1150 |
| FC000001793 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4655 | 1 | 1158 |
| FC000001794 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 3790 | 1 | 946 |
| FC000001795 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4540 | 1 | 1118 |
| FC000001796 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4160 | 1 | 1036 |
| FC000001832 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 3240 | 1 | 798 |
| FC000001973 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4510 | 1 | 1110 |
| FC000001974 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4730 | 1 | 1166 |
| FC000002393 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4625 | 1 | 1140 |
| FC000004923 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 3956.6 | 1 | 1006 |
| FC000004931 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4765 | 1 | 1184 |
| FC000004938 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 5435 | 1 | 1352 |
| FC000004939 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4675 | 1 | 1158 |
| FC000004943 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 3595 | 1 | 894 |
| FC000004955 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 5920 | 1 | 1466 |
| FC000004956 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 5995 | 1 | 1494 |
| FC000004961 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 4690 | 1 | 1170 |
| FC000004965 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 2625 | 1 | 654 |
| FC000004975 | 1.2379 | Round Bar | Turned | EF+LF+VD | 202 | 2620 | 1 | 652 |
| FC000002026 | 1.2379 | Round Bar | Turned | EF+LF+VD | 210 | 5067.4 | 1 | 1392 |
| FC000004982 | 1.2379 | Round Bar | Turned | EF+LF+VD+ESR | 210 | 4718 | 1 | 1296 |
| FC000001248 | 1.2379 | Round Bar | Turned | EF+LF+VD | 212 | 4200 | 1 | 1160 |
| FC000003300 | 1.2379 | Round Bar | Turned | EF+LF+VD | 220 | 3006.5 | 1 | 906 |
| FC000008200 | 1.2379 | Round Bar | Turned | EF+LF+VD | 220 | 4190 | 1 | 1258 |
| FC000008319 | 1.2379 | Round Bar | Turned | EF+LF+VD | 220 | 2820 | 1 | 858 |
| FC000004927 | 1.2379 | Round Bar | Turned | EF+LF+VD | 222 | 4965 | 1 | 1484 |
| FC000004945 | 1.2379 | Round Bar | Turned | EF+LF+VD | 222 | 5065 | 1 | 1516 |
| FC000004948 | 1.2379 | Round Bar | Turned | EF+LF+VD | 222 | 5125 | 1 | 1532 |
| FC000004953 | 1.2379 | Round Bar | Turned | EF+LF+VD | 222 | 4975 | 1 | 1486 |
| FC000004980 | 1.2379 | Round Bar | Turned | EF+LF+VD+ESR | 230 | 4680 | 1 | 1518 |
| FC000008244 | 1.2379 | Round Bar | Turned | EF+LF+VD | 230 | 5160 | 1 | 1704 |
| FC000007158 | 1.2379 | Round Bar | Turned | EF+LF+VD | 240 | 2578.4 | 1 | 924 |
| FC000008318 | 1.2379 | Round Bar | Turned | EF+LF+VD | 240 | 2150 | 1 | 780 |
| FC000001840 | 1.2379 | Round Bar | Turned | EF+LF+VD | 242 | 5090 | 1 | 1808 |
| FC000004922 | 1.2379 | Round Bar | Turned | EF+LF+VD | 242 | 4300 | 1 | 1522 |
| FC000005002 | 1.2379 | Round Bar | Turned | EF+LF+VD | 242 | 4140 | 1 | 1474 |
| FC000007078 | 1.2379 | Round Bar | Turned | EF+LF+VD | 250 | 2510.8 | 1 | 976 |
| FC000002747 | 1.2379 | Round Bar | Turned | EF+LF+VD | 260 | 4097 | 1 | 1722 |
| FC000001969 | 1.2379 | Round Bar | Turned | EF+LF+VD | 262 | 5260 | 1 | 2180 |
| FC000001970 | 1.2379 | Round Bar | Turned | EF+LF+VD | 262 | 5160 | 1 | 2144 |
| FC000001971 | 1.2379 | Round Bar | Turned | EF+LF+VD | 262 | 4840 | 1 | 2008 |
| FC000002394 | 1.2379 | Round Bar | Turned | EF+LF+VD | 262 | 5390 | 1 | 2238 |
| FC000008643 | 1.2379 | Round Bar | Turned | EF+LF+VD | 280 | 4625 | 1 | 2246 |
| FC000008644 | 1.2379 | Round Bar | Turned | EF+LF+VD | 280 | 4625 | 1 | 2248 |
| FC000004979 | 1.2379 | Round Bar | Turned | EF+LF+VD+ESR | 330 | 4449.8 | 1 | 3008 |
| FC000004990 | 1.2379 | Round Bar | Turned | EF+LF+VD+ESR | 360 | 4365 | 1 | 3410 |
1.2379 Round Bar-Grinded
FCS Tool Steel Manufacturer Stocklist(2025.07.31) |
||||||||
Stock No. |
Grade |
Shape |
Surface |
Process |
Thickness/Diameter |
Length |
PCS |
Weight(KG) |
| FC000003095 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 70 | 2189.8 | 1 | 72 |
| FC000003563 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 80 | 1882.1 | 1 | 80 |
| FC000003079 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 100 | 2665 | 1 | 192 |
| FC000003277 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 130 | 4805 | 1 | 554 |
| FC000003084 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 200 | 3045 | 1 | 764 |
| FC000003099 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 200 | 4305 | 1 | 1090 |
| FC000003101 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 200 | 4980 | 1 | 1320 |
| FC000007844 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 200 | 4490 | 1 | 1138 |
| FC000005989 | 1.2379 | Round Bar | Grinded | EF+LF+VD | 210 | 4244 | 1 | 1188 |
Additional information
| Weight | 45 kg |
|---|---|
| Dimensions | 165 × 60 × 25 cm |















-1-300x300.png)