1.2358 | X60CrMoV18-5 Tool Steel
Supply Condition:Annealed,Machined
Available Forms:Round bars,Plates / Flat bars,Custom-cut pieces
Processing Services:Sawing,Rough machining,Custom heat treatment.
Standard Size Range (Availability varies by stock):
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
Forming Methods:Hot Rolled,Hot Forged.
Surface Finish Options:Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
1.2358 | X60CrMoV18-5 Tool Steel:Overview of Materials

1.2358 | X60CrMoV18-5 Tool Steel is a high-performance German DIN standard cold work tool steel, designed for demanding applications requiring both strength and wear resistance. With a balanced alloy composition of approximately 1.28-1.62% carbon, 10.5-12% chromium,0.55-0.95% molybdenum, and vanadium additions, it combines excellent hardness retention at elevated temperatures with superior resistance to thermal fatigue and oxidation.
This steel grade exhibits outstanding toughness and dimensional stability during heat treatment, making it well suited for long-life tools exposed to mechanical and thermal stress. It also provides enhanced corrosion resistance compared to conventional hot work steels, thanks to its high chromium content.
Typical applications include die-casting molds, hot shear blades, forging dies, and extrusion tools where both wear resistance and heat resistance are critical. Its reliable performance and reduced maintenance requirements make 1.2358 an excellent choice for industries such as automotive, aerospace, and heavy manufacturing.
1.2358 | X60CrMoV18-5:Product Specification

1.2358 | X60CrMoV18-5 Tool Steel:Chemical Composition

1.2358 | X60CrMoV18-5 Tool Steel:International and grade comparison

1.2358 | X60CrMoV18-5 Tool Steel:Surface Condition

1.2358 | X60CrMoV18-5 Tool Steel:Milled plate

1.2358 | X60CrMoV18-5 Tool Steel:Turned and Peeled Round Steel

1.2358 | X60CrMoV18-5 Tool Steel:Sandblasted Round Bar

Additional information
| Weight | 2 kg |
|---|---|
| Dimensions | 10 × 20 × 15 cm |