Sale!

3Cr17 Tool Steel

The international approximate/corresponding grades of 3Cr17 Tool Steel include DIN 1.2085 (a common counterpart) and JIS SUS420F (or similar to the 420-series martensitic stainless steels).Common similar designations: 3Cr17, 3Cr17+S (sulfur-containing free-cutting grade).These correspondences are functional approximations, not identical in terms of chemical composition and manufacturing processes. When selecting alternative materials, please compare the chemical composition, hardness, and end-use application.

Process:EF+LF+VD+Hot rolled /Hot Forged+Annealing

Surface condition: Black,Peeled; Polished,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

Delivery condition: Hot Forged,Hot Rolled,Annealed

Available Forms:Round bars,Plates / Flat bars,Custom-cut pieces

Processing Services:Sawing,Rough machining,Custom heat treatment.

Payment terms: T/T;L/C

Trade terms: FOB,CIF,CFR,etc..

Standard Size Range (Availability varies by stock):

  1. Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
  2. Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
  3. Width: 50 – 1000 mm / 50 – 1500 mm.
  4. Forged Discs: Up to Ø1200 mm.
Categories: , Tags: , ,

What is 3Cr17 Tool Steel?

What is 3Cr17 Tool Steel?

3Cr17 (sometimes written as 3Cr17+S) is a martensitic stainless tool steel/mold steel. It contains approximately 15% chromium, can be quenched and tempered to achieve medium-to-high hardness, and is commonly used in scenarios such as injection molds, cold work molds, cutting tools, and mechanical parts. When marked with "S", it is a free-cutting grade (containing sulfur) with improved machinability.

3Cr17 Tool Steel:Product Specification

3Cr17 Tool Steel:Product Specification

3Cr17 Tool Steel:Chemical Composition

Chemical Composition:3Cr17 Tool Steel,3Cr17+S,SUS420F,1.2085

3Cr17 Tool Steel:International and grade comparison

3Cr17 Tool Steel:International and grade comparison

3Cr17 Tool Steel:Surface Condition

3Cr17 Tool Steel:Surface Condition

3Cr17 Tool Steel:Milled plate

3Cr17 Tool Steel:Milled plate

3Cr17 Tool Steel:Turned and Peeled Round Steel

3Cr17 Tool Steel:Turned and Peeled Round Steel

3Cr17 Tool Steel:Sandblasted Round Bar

3Cr17 Tool Steel:Sandblasted Round Bar

 

Additional information

Weight 30 kg
Dimensions 180 × 120 × 18 cm