1.2362 Tool Steel
At FCS Tool Steel, we offer 1.2362 Tool Steel in multiple supply conditions:
Supply Condition:Annealed,Machined
Available Forms:Round bars,Plates / Flat bars,Custom-cut pieces
Processing Services:Sawing,Rough machining,Custom heat treatment.
Standard Size Range (Availability varies by stock):
- Diameter (Round bar): Φ10 mm – Φ65 mm / Φ70 mm – Φ400 mm / Φ500 mm / Φ600 mm / Φ700 mm.
- Plate/Flat Thickness: 8 – 45 mm / 50 – 500 mm.
- Width: 50 – 1000 mm / 50 – 1500 mm.
- Forged Discs: Up to Ø1200 mm.
Forming Methods:Hot Rolled,Hot Forged.
Surface Finish Options:Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
1.2362 Tool Steel:Material positioning

1.2362 (X63CrMoV5-1) is a Cr-Mo-V alloy cold working tool steel, featuring high tempering resistance and good hardenability. It is often used for tool and die components that are subject to impact and wear and require stable hardness. It is also seen in the application of cutting edge materials in working conditions such as thermal shearing and trimming.
1.2362 Tool Steel:Product Specification

1.2362 Tool Steel:Chemical Composition

1.2362 Tool Steel:International and grade comparison

1.2362 Tool Steel:Surface Condition

1.2362 Tool Steel:Milled plate

1.2362 Tool Steel:Turned and Peeled Round Steel

1.2362 Tool Steel:Sandblasted Round Bar

1.2362 Tool Steel:Typical physical/mechanical indicators (examples)
- Density: Approximately 7.8 g/cm³.
- Elastic modulus: approximately 210 GPa.
- State hardness: annealed state ≲~230 HB; After quenching, it is common to have adjustable HRC ranging from 58 to 62.
Additional information
| Weight | 45 kg |
|---|---|
| Dimensions | 165 × 135 × 25 cm |



-1.webp)