2750 Tool Steel

2750 is commonly used in Sweden or ASSAB/Uddeholm to identify a high performance high-speed steel, corresponding to P18 or DIN/W-Nr S18-0-1/1.3355 internationally. This type of steel is renowned for its high toughness and superior red hardness, and is suitable for high-speed cutting tools that require maintaining hardness, heat resistance and wear resistance. It performs stably at high temperatures and is particularly suitable for long-life cutting tools and cutting tools for difficult-to-cut materials.

2750 Tool Steel Size Range

  1. 2750 Hot Rolled Plate/Flat Bar:Thickness: 10-400mm,Width: 200-800mm,Length: 3000-5800mm
  2. 2750 Hot Forged Plate/Flat Bar:Thickness: 50-500mm,Width: 50-1500mm,Length: 3000-5800mm
  3. 2750 Hot Rolled Round Bar: Diameter 10-65mm,Length 3000-5800mm
  4. 2750 Hot Forged Round Bar:Diameter:70-700mm,Length:3000-5800mm

2750 Tool Steel Surface Finish

Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

2750 Tool Steel Chemical Composition

2750 Tool Steel Chemical Composition

2750 Tool Steel Equivalent Grades

2750 Tool Steel Equivalent Grades

2750 Tool Steel Specifications

Tool Steel Specifications

2750 Tool Steel Customized Options

 Tool Steel Customized Options

  1. Custom Surface Conditions: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
  2. Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
  3. Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
  4. Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
  5. Custom production according to samples or technical agreements.
  6. 2750 Tool Steel Electroslag Remelting (2750 ESR): Premium option with higher purity and isotropic properties for critical applications.

2750 Tool Steel Smelting process

Tool Steel Smelting process

2750 Tool Steel Physical Properties

 Tool Steel Physical Properties

  1. Density: approximately 7.0-7.5 kg/dm³.
  2. Tensile strength (Rm) : ≥ 592 MPa; Yield strength (Rp₀.₂) : ≥ 191 MPa.
  3. Impact toughness (Charpy KV) : approximately 32 J; Elongation and reduction of area are both lower than 50 %.
  4. Factory hardness: approximately HB 310-320 (approximately HRC 30).
  5. Thermal performance: The thermal diffusivity, thermal conductivity and thermal expansion rate are all suitable for long-term application under thermal load conditions.

2750 Tool Steel Mechanical & Performance Properties

Tool Steel Mechanical & Performance Properties

  1. Extremely high wear resistance: Due to the uniform network structure formed by tungsten, molybdenum and vanadium carbides, it is very suitable for long-term continuous cutting use.
  2. Good impact toughness: Unlike many hard steels, it still retains a certain degree of plasticity in a high-hardness state.
  3. Strong thermal stability: It is not prone to deformation at high temperatures and its hardness remains stable.
  4. Solderability and repairability: Official data also indicates that it can be repaired by welding or partially reconstructed.

2750 Tool Steel Product Applications

Tool Steel Product Applications

Suitable for making tools that require extreme wear resistance and high-temperature stability, such as:

  1. Single-edge drill bits, hobs, small punching and shearing tools.
  2. High-temperature cutting components of special materials.
  3. High-speed metal cutting and graphite/composite material processing tools, etc.

For industrial use: In environments with high requirements for tool life and large heat loads.