P18 Tool Steel
P18 (R18) high-speed steel is a classic and high-performance steel grade with high hardness, high red hardness and high wear resistance. It combines excellent toughness and resistance to hot cracking, making it suitable for a variety of high-strength cutting and cold working tools. It has wide international equivalence, mature smelting technology, stable and reliable performance, and is a highly cost-effective choice in engineering and manufacturing.
P18 Tool Steel Size Range
- Hot Rolled Plate/Flat Bar:Thickness: 10-400mm,Width: 200-800mm,Length: 3000-5800mm
- Hot Forged Plate/Flat Bar:Thickness: 50-500mm,Width: 50-1500mm,Length: 3000-5800mm
- Hot Rolled Round Bar: Diameter 10-65mm,Length 3000-5800mm
- Hot Forged Round Bar:Diameter:70-700mm,Length:3000-5800mm
P18 Tool Steel Surface Finish
Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
P18 Tool Steel Chemical Composition

P18 Tool Steel Equivalent Grades

The approximate correspondence of P18 in the standards of various countries is as follows:
- Russia (GOST): P18 tool steel
- China (GB): W18Cr4V tool steel
- Germany (DIN / W-Nr):S18-0-1/1.3355
- Japan (JIS): SKH2 tool steel
- USA (AISI/ASTM):T1 tool steel
- Sweden (ASSAB): 2750 tool steel
P18 Tool Steel Specifications

P18 Tool Steel Customized Options

- Custom Surface Conditions: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
- Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
- Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
- Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
- Custom production according to samples or technical agreements.
- P18 Tool Steel Electroslag Remelting (P18 ESR): Premium option with higher purity and isotropic properties for critical applications.
P18 Tool Steel Smelting process

P18 Tool Steel Physical Properties

- Density: ≈ 8800 kg/m³
- Modulus of elasticity: ≈ 228 GPa at 20°C, decreasing to about 180 GPa at 600°C.
- Thermal conductivity: 20℃≈26 W/(m-K), 400-600℃≈29-27 W/(m-K)
- Specific heat capacity: 20 ℃ ≈ 419 J / (kg - K); with the rise in temperature increases gradually
- Resistivity: 20℃ ≈419 nΩ-m, to 600℃ ≈922 nΩ-m
P18 Tool Steel Mechanical & Performance Properties

- High hardness: After quenching (oil quenching at 1280℃), the hardness can reach 61-66 HRC. The higher the tempering temperature, the lower the hardness but the higher the toughness. Typically, it is about 65 HRC.
- Excellent red hardness: It remains stable at high hardness up to 600℃, making it suitable for high-speed cutting environments.
- Combining wear resistance and toughness: High tungsten and vanadium elements form hard carbides, which also have sufficient toughness to be suitable for impact environments.
- Excellent thermal crack resistance: It has good thermal stability after heat treatment and outstanding crack resistance.
P18 Tool Steel Product Applications

- Cutting tools: milling cutters, drills, taps, reamers, etc.
- Precision tools: forming tools, gear shaping tools and tool blanks.
- Cold working dies: used for stamping, cutting, punching and blade manufacturing.
- High-temperature rolling and cutting applications: It performs exceptionally well in environments with high heat resistance requirements.