In mid-2025, the global tool steel market will face a new wave of volatility, primarily driven by the sharp rise in the prices of tungsten (W) and molybdenum (Mo) alloys. For tool steel buyers, this means not only increased procurement costs but also the need for more strategic purchasing decisions to ensure stable supply and cost control. This guide will walk you through the impact of the alloy price surge, which tool steel grades are most affected, and practical procurement strategies — including the rare opportunity for FCS tool steel to clear its inventory starting from July 2025 and still ongoing.

Why Alloy Prices Are Soaring in 2025
In July 2025, the prices of tungsten and molybdenum alloys began climbing rapidly. Factors such as global supply constraints, increased demand in aerospace and defense industries, and rising mining costs are pushing the market upward. Since both tungsten and molybdenum are critical alloying elements in many high-performance tool steels, their price surge directly translates into higher manufacturing costs for these steels.
Tool Steel Grades Most Affected by the Price Hike
The most impacted tool steels are those with high W or Mo content:
High Tungsten (W) Grades:
High Molybdenum (Mo) Grades:
These grades are widely used in mold making, precision tooling, and high-wear applications. With rising raw material costs, their market prices are expected to stay elevated for a considerable time.
Procurement Strategies in a Price Surge
- In this volatile market, steel buyers can consider the following approaches:
- Advance Purchases: Secure stock ahead of further price hikes.
- Seek Clearance Sales: Monitor market offers from suppliers liquidating inventory.
- Diversify Grades: Where feasible, opt for grades with lower W and Mo content to control costs.
- Partner with Reliable Suppliers: Ensure consistent quality and delivery even when the market is tight.
FCS Tool Steel’s August 2025 Clearance Sale — A Buyer’s Opportunity
As tungsten and molybdenum prices continue to rise, FCS Tool Steel has launched a August 2025 inventory clearance sale to help buyers secure high-quality stock at competitive prices before further market increases.
Clearance inventory includes:
1.2344 Tool Steel

- Plate: Turned surface / Black surface
- Round bar: Grinded surface / Turned surface
1.2379 Tool Steel

- Plate: Turned surface / Black surface
- Round bar: Grinded surface / Turned surface
1.2316 Tool Steel

- Plate: Black surface
- Round bar: Grinded surface / Turned surface
D2 Tool Steel

- Plate: Turned surface / Black surface
- Round bar: Grinded surface / Turned surface
SKD11 Tool Steel

- Plate: Turned surface / Black surface
- Round: Grinded surface / Turned surface / Black surface
Advantages of this clearance:
- Immediate Delivery: All items are in stock and ready to ship.
- Multiple Specifications: Covers a wide range of sizes and processing states.
- Competitive Pricing: Ideal for bulk buyers during the alloy price surge.
For mold manufacturers, tooling companies, and distributors, this clearance is a rare chance to lock in cost advantages before the market reaches new highs.
Final Advice
The alloy price surge in 2025 is a reminder that raw material volatility is now a constant risk in the tool steel market. Buyers should combine market intelligence with flexible procurement strategies and seize opportunities like FCS Tool Steel’s August clearance to secure both supply stability and cost competitiveness.In an unpredictable market, the smartest buyer isn’t just the one who negotiates well — it’s the one who buys at the right time.
summary
From my experience, smart buying is about more than just finding the lowest price. I’ve learned it comes down to good timing, solid preparation, and building strong supplier partnerships. The market is always changing. I believe the companies that will do well are the ones that act quickly on opportunities. A great example is the current clearance sale at FCS Tool Steel. The 2025 alloy surge presents a real challenge. I see it as a chance to become a better buyer, forcing me to plan for the future instead of just focusing on today.