S136H Tool Steel
S136H is a pre-hardened mirror-finish plastic mold steel launched by ASSAB of Sweden, belonging to the high-chromium stainless alloy series. Its hardness is approximately HRC 30-36 in the factory state and it can be used without heat treatment. It is especially suitable for plastic molds in damp or corrosive environments. This steel has excellent mirror polishing performance and outstanding corrosion resistance and wear resistance.
S136H Tool Steel Size Range
- Hot Rolled Plate/Flat Bar:Thickness: 10-400mm,Width: 200-800mm,Length: 3000-5800mm
- Hot Forged Plate/Flat Bar:Thickness: 50-500mm,Width: 50-1500mm,Length: 3000-5800mm
- Hot Rolled Round Bar: Diameter 10-65mm,Length 3000-5800mm
- Hot Forged Round Bar:Diameter:70-700mm,Length:3000-5800mm
S136H Tool Steel Surface Finish
Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.
S136H Tool Steel Chemical Composition

S136H Tool Steel Equivalent Grades

The approximate correspondence of S136H in the standards of various countries is as follows:
- China (GB):3Cr17NiMo
- Germany (DIN / W-Nr):X36CrMo17/1.2316
- Austria(BOHLER):M300
- USA (AISI/ASTM):420H
- Sweden (ASSAB):S136H Tool Steel
S136H Tool Steel Specifications

S136H Tool Steel Customized Options

- Custom Surface Conditions: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
- Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
- Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
- Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
- Custom production according to samples or technical agreements.
- S136H Tool Steel Electroslag Remelting (S136H ESR): Premium option with higher purity and isotropic properties for critical applications.
S136H Tool Steel Smelting process

S136H Tool Steel Physical Properties

- Density: approximately 7.85 kg/dm³
- Elastic modulus: approximately 215 GPa (20 °C)
- Coefficient of thermal expansion: approximately 11×10⁻⁶/K
- Thermal conductivity: approximately 32-33 W/m·K
- Yield strength Rp₀.₂ : ≥593 MPa; Tensile strength Rₘ ≥526 MPa; Impact toughness ≈42 J; Annealing hardness is approximately HB 313.
S136H Tool Steel Mechanical & Performance Properties

- Excellent corrosion resistance: The high-chromium formula performs outstandingly in environments containing PVC, vinyl acetate, and food-grade plastics, ensuring that the mold surface remains rust-free for a long time.
- Outstanding mirror polishing performance: polishing can reach Ra ≤ 0.01 μm, suitable for optical molds and transparent product molds.
- Wear-resistant and with moderate hardness: The factory hardness is 30-36 HRC, and it can work within the 48-52 HRC range as required by processing. It has both wear-resistant and crack-resistant capabilities.
- Good machinability: Compared with common hardened steel, it has a fast processing speed and is easy to be boring, milling, EDM and polished.
S136H Tool Steel Product Applications

- Optical plastic product molds (such as camera lenses, sunglasses, medical device shells).
- Corrosive plastic injection molds such as PVC, PP, EP, PC, PMMA, etc.
- Food-grade or medical device molds (disposable tableware, instrument components).