M310 Tool Steel

M310 Tool Steel corresponds to grades such as 1.2083, 420SS , SUS420J2 ,4Cr13 ,40X13,X42Cr13,S136, etc. in multiple global standards.

Supply status and size specifications of M310

  1. M310 Delivery condition: Annealed state (HB ≤225)
  2. M310 Supply forms: round steel, flat steel, plates, forgings, custom cutting
  3. M310 Optional sizes: Diameter Φ10 ~ Φ65/Φ 70 ~ Φ400/500/600/700 mm,thickness 8-45/50-500mm,width 50-1000mm/50-1500mm, Forged disc ≤ 1200mm,
    etc

M310 Tool Steel Forming Process Options

M310 Hot Rolled,M310 Hot Forged

M310 Tool Steel Surface Finish

Black,Grinded,Sandblasted,Turned/Machined/Milled/Bright.

What is M310 tool steel?

BOHLER M310 is a high-chromium plastic tool steel that combines high polishing, corrosion resistance and machinability, corresponding to multiple national standards (such as S136 / ASTM 420SS / SUS420J2). It has advantages in the field of food-grade plastic molds and is particularly suitable for working conditions that require smooth mold surfaces, high corrosion resistance and low processing stress.

What are the specifications of M310 tool steel?

Specifications : M310 tool steel

What are the Equivalent Grades of M310 Tool Steel?

the Equivalent Grades of M310 Tool Steel

What is the Chemical Composition of M310 Tool Steel?

 the Chemical Composition of M310 Tool Steel

What are the Customized Options of M310 Tool Steel ?

  1. Custom Chemical Composition: Capable of producing standard grades such as GB, DIN, ASTM, JIS, etc. Chemical composition can be custom-produced individually.
  2. Custom Specifications: Round steel (diameter) and plates (thickness, width) can be custom-produced.
  3. Professional packaging for long-term storage or extreme transportation conditions: Including black paint spraying on all sides, plastic film wrapping, anti-rust oil spraying, and delivery in wooden cases.
  4. Custom production according to samples or technical agreements.
  5. M310 Tool Steel Electroslag Remelting (M310 ESR): Premium option with higher purity and isotropic properties for critical applications.

What is the Smelting process of M310 Tool Steel ?

Tool Steel Smelting process:M310

M310 Tool Steel Physical properties

  1. Extremely high processability.
  2. Excellent dimensional stability.
  3. Good polishing property (especially suitable for high-gloss mold surfaces).
  4. Strong corrosion resistance (due to high chromium content).
  5. High microscopic purity.

M310 Tool Steel Typical application fields

Tool Steel Product Applications

  1. High-gloss injection molds, hot runner system components, and precision blow-molded parts.
  2. Processing molds for food, beverages and medical plastic products.
  3. Electronic product lens housings, display components, thermoplastic molds.
  4. Ordinary mechanical parts, standard mold components (plates, pins, pins, etc.) involve scenarios with high cleanliness or high corrosion resistance requirements.