1.2344
1.2344 Hot Work Tool Steel is a chromium-molybdenum-vanadium alloy steel, featuring excellent high-temperature strength, wear resistance, and thermal fatigue resistance. It can maintain good toughness and dimensional stability at high temperatures, with strong cracking resistance and stable heat treatment performance. 1.2344 is widely used in the manufacturing of tools and molds for high-temperature working conditions, such as die-casting molds for aluminum, magnesium, and copper alloys, hot forging dies, extrusion dies, and hot shear blades. It is one of the classic high-performance materials in the field of hot work molds.