O1|1.2510|DF-3|K460|SKS3|100MnCrW4|9XBГ|9CrWMn

Surface Condition:Black; Peeled/Grinded; Turned/Machined/Bright/Milled

  1. O1 Tool Steel (AISI/SAE):Up to 62–64 HRC after heat treatment.
  2. 1.2510 (DIN, German Equivalent of O1):Oil-hardening cold-work steel (similar to AISI O1).60–63 HRC
  3. DF-3 (Daido Steel, Japan):High-carbon, high-chromium cold-work steel.
  4. K460 (BOHLER, Austria):High-performance cold-work steel.
  5. 100MnCrW4 (DIN, German):Manganese-chromium-tungsten cold-work steel.
  6. 9XBΓ (Russian/Former Soviet Union, Equivalent to 9CrWMn):Chromium-tungsten-manganese cold-work steel.
  7. 9CrWMn Steel (GB, China):Low-alloy cold-work steel (equivalent to 9XBΓ and AISI O7).

 

SKU: N/A Category: Tags: , , , , , , , ,
Equivalent grades of 1.2510 tool steel: AISI O1 (US), JIS SKS3 (Japan), GB CrWMn (China), BS O1 (UK), NF 90MnCrV8 (France), UNI C90MnCrV8 (Italy), ISO 4957/X90MnCrV8.The main differences between 1.2510 and 1.2601 (equivalent to A2 etc.) lie in properties. 1.2510 is oil – hardening with good machinability and moderate wear resistance. 1.2601 is air – hardening, offering better dimensional stability, higher wear resistance, and better toughness. Their different alloy compositions lead to distinct heat – treatment responses and application scopes.
AISI / ASTM O1 Tool Steel is a low alloy cold work tool steel that must be oil-quenched in heat treatment. Tools and dies made from O1 tool steel flat or rounds will have good wearing and abrasive qualities since the tungsten and higher chromium content gives improved wear resistance.ASTM O1 tool steel has deep hardening properties with fine grain structure with unusual toughness. AISI O1 tool steel offers good durability, gives excellent wear resistance and holds a good cutting edge. O1 cold work tool steels also has good response to heat treatment with small dimensional changes.We are a better choice of O1 oil tool steel materials supplier with reliable quality and sales service. AISI Tool steel O1 is available in standard de-carb free rounds, flats and squares, as well as the largest size selection in O1 oil steel ground flat stock and drill rod of all the tool steel grades, or as per customized requirements.

O1|1.2510|K460|SKS3|100MnCrW4|9XBГ|9CrWMn|

DF-3

Smelting and Manufacture Method: LF+VD+Forged
Delivery Condition: Annealed
Delivery hardness: ≤230 HBS
UT Test Standard: Sep 1921-84 Class3 D/d,E/e
Brand Fucheng steel
Product origin China
Supply capacity 2000 Tons/Month

Supply Form & Range

For 1.2510|O1|K460|SKS3|100MnCrW4|9XBГ|9CrWMn|DF-3 steel, we can provide round bars and plates. Round rods can be sawn to the length you need and used as single or multiple cut pieces. Grinding tool steel bars can be provided, offering high-quality precision finished bars for strict tolerances.

In addition, we can provide a variety of surface conditions of tool steels:BlackPeeled/Grinded;Turned/Machined/Bright/Milled

Product Type Dimensions Range
Round Bar Diameter 16 – 400 mm
Length 3,000 – 5,800 mm
Flat Bar Thickness 16 – 300 mm
Width 200 – 800 mm
Length 3,000 – 5,800 mm

Chemical Composition

O1/1.2510/SKS3/100MnCrW4

Standard/Steel Grade Chemical Composition(%)
C Si Mn Cr V W
ASTM O1 0.85~1.00 0.10~0.50 1.00~1.40 0.40~0.60 ≤0.30 0.40~0.60
DIN/W-Nr. 100MnCrW4/1.2510 0.90~1.05 0.15~0.35 1.00~1.20 0.50~0.70 0.05~0.15 0.50~0.70
JIS SKS3 0.90~1.00 ≤0.35 0.90~1.20 0.50~1.00 - 0.50~1.00

APPLICATION

1.2510 tool steel is used a lot for blanking and punching dies. Its strength helps it handle heavy-duty tasks. This steel works well in applications needing long-lasting performance and precise cuts. It’s commonly chosen for manufacturing dies due to its reliability in tough conditions.

Steel Grade Primary Applications
O1 Cutting tools, gauges, punches, dies, woodworking tools, and precision measurement tools.
1.2510 Blanking dies, forming tools, shear blades, and wear-resistant industrial components.
DF-3 Plastic molds, cold-forming dies, slitting knives, and thread-rolling dies.
K460 Precision stamping dies, forming tools, and high-wear resistance components.
SKS3 Press dies, punches, cutting blades, and small precision molds requiring toughness.
100MnCrW4 Cold extrusion tools, cutting dies, and wear-resistant parts for industrial machinery.
9XBГ (9KhVG) Cold-work punches, forming dies, and shear blades in heavy-duty applications.
9CrWMn Cold stamping dies, trimming tools, and wear-resistant components requiring high hardness.

Reviews

There are no reviews yet.

Be the first to review “O1|1.2510|DF-3|K460|SKS3|100MnCrW4|9XBГ|9CrWMn”

Your email address will not be published. Required fields are marked *