H13 / SKD61 / 1.2344 / 4Cr5MoSiV1 / 8407 / W302 / 4X5MΦ1C / X40CrMoV5-1:Ideal for die forging and hammer forging dies, our H13 steel ensures superior performance in high-temperature environments. It is perfect for aluminum alloy die casting, hot extrusion dies, and high-speed precision forging applications.
This category belongs to chromium-molybdenum series hot work die steels, which are widely used hot work tool steels. They exhibit excellent toughness, thermal fatigue resistance, and wear resistance, along with good hardenability and tempering stability. These steels excel in manufacturing die-casting molds for aluminum, magnesium, zinc alloys, and are also suitable for hot forging dies, hot extrusion dies, and precision forging dies.
4X5MΦ1C Steel
This is a Russian hot work die steel equivalent to China's 4Cr5MoSiV1. It features good toughness and thermal strength, capable of maintaining high hardness at elevated temperatures. Applications include hot forging dies, die-casting dies, and hot extrusion dies.
X40CrMoV5-1 Steel
This is a German hot work die steel comparable to China's 4Cr5MoSiV1. It boasts high thermal strength, hardness, excellent thermal fatigue resistance, and good hardenability. It is suitable for manufacturing hot forging dies, die-casting dies, hot extrusion dies, and high-speed precision forging dies.
For H13 | SKD61 | 1.2344 | 4Cr5MoSiV1 | 8407 | W302 | 4X5MΦ1C | X40CrMoV5-1 steel, we can provide round bars and plates. Round rods can be sawn to the length you need and used as single or multiple cut pieces. Grinding tool steel bars can be provided, offering high-quality precision finished bars for strict tolerances.
Product Type
Dimensions
Range
Round Bar
Diameter
16 – 400 mm
Length
3,000 – 5,800 mm
Flat Bar
Thickness
16 – 300 mm
Width
200 – 800 mm
Length
3,000 – 5,800 mm
In addition, we can provide a variety of surface conditions of tool steels:Black;Peeled/Grinded;Turned/Machined/Bright/Milled