1.2316 Tool Steel

Designed for superior acid resistance and polishability, FCS Factory offers high quality 1.2316 tool steel that maintains dimensional stability and excellent machinability for superior performance in harsh environments.

1.2316 Tool Steel Product Description

1.2316 tool steel1.2316 tool steel

1.2316 tool steel is a martensitic stainless chromium-molybdenum steel that belongs to the German DIN standard (e.g. EN 10088: X36CrMo17) for high-alloyed tool steels with excellent corrosion resistance, high hardness and mirror-polishing properties. Its core strength is its resistance to corrosive environments such as acids, alkalis or salts, which makes it particularly suitable for the manufacture of molds that come into contact with corrosive plastics (e.g. PVC).
In harsh processing environments where standard tool steels fail quickly and manufacturers face high downtime costs and quality issues, FCS Factory offers DIN 1.2316 tool steel to address these challenges through optimized chromium content (16-18%) and specialized heat treatments. Meanwhile, FCS TOOL STEEL as a professional tool steel supplier and manufacturer, we offer 1.2316 tool steel in various stock forms.

1.2316 Tool Steel Product Types and Options

Rolled round steelSteel Milled surface

As a vertically integrated supplier of specialty steels, FCS TOOL STEEL is able to respond quickly to customized needs with a fully integrated production line and a 1.2316 stockpile, which is often used by manufacturers to obtain high-precision die steels that are subject to fluctuating delivery schedules and insufficient material preparation.
The 1.2316 product offering at FCS Plant covers both round and plate forms. Round steel is available in both hot rolled and hot forged, while plate is available in both hot rolled and hot forged. Below is a detailed list of 1.2316 specifications, surface treatments and accuracy controls:

Shape Pocess Size range Surface Tolerance
Flat Bar Hot Rolled Thickness: 10-400mm

Width: 200-800mm

Length: 3000-5800mm

Black;

Sandblasted

Thickness :0-+2MM

Width:0-+5MM/0-+10MM

Hot Forged Thickness: 50-500mm

Width: 50-1500mm

Length: 3000-5800mm

Black Thickness:+2-+5MM

Width:0-+5MM/0-+10MM

Turned/Machined/Milled/Bright Thickness :0-+2MM

Width:0-+5MM/0-+10MM

Round Bar

 

Hot Rolled Diameter:10-65mm

Length:3000-5800mm

Black 0-+2MM
Turned/Machined 0-+2MM
Hot Forged Diameter:70-700mm

Length:3000-5800mm

Grinded 0-+5MM/+2-+5MM
Turned/Machined/Milled/Bright 0-+2MM

1.2316 STEEL Customization Options

tool steel surface conditionTurning smooth round steel

  1. Customized surface condition: Black; Sandblasted; Grinded; Turned/Machined/Milled/Bright
  2. Customized chemical composition: GB, DIN, ASTM, JIS and other standard grades can be produced. Chemical composition can be customized individually.
  3. Customized specifications: round steel (diameter), plate (thickness, width) can be customized production.
  4. Specialized packaging for long term storage or extreme transportation conditions: includes spraying black paint all around, wrapping plastic film, spraying anti-rust oil, and shipping in wooden crates.
  5. Customized production based on samples or technical agreements.
  6. 1.2316 Electroslag Remelting (ESR): premium option with higher purity and isotropic properties for critical applications.

1.2316 Tool Steel Chemical Composition

1.2316 Tool Steel
Tool Steel Grade Chemical Composition(%)
C Si Mn Cr Mo Ni
DIN/W-Nr. X36CrMo17/1.2316 0.33~0.43 ≤1.00 ≤1.00 15.0~17.0 1.00~1.30 ≤1.00
GB 3Cr17NiMo 0.28~0.35 ≤0.80 ≤1.00 16.0~18.0 0.75~1.25 0.6~1.00

1.2316 Tool Steel Heat treatment process

Vacuum degassing(VD)

1.Annealing

Purpose: to eliminate internal stresses generated during forging or rolling, reduce hardness, improve cutting performance, and prepare for subsequent processing and heat treatment.
Process parameters:
Heating temperature: 800-850 ℃, holding time 2-4 hours, with the furnace cooling to below 500 ℃, and then air-cooled.
Hardness after annealing: ≤ 250 HBS.

2.Quenching

Purpose: to make the steel to obtain martensitic organization, improve hardness and wear resistance.
Process parameters:
Heating temperature: 1000-1050 ℃ (commonly used 1020-1040 ℃), holding time according to the size of the workpiece to determine, generally 30-60 minutes.
Cooling: oil cooling or air cooling (for small size or simple shape of the workpiece), large workpieces can be graded quenching (in the 260-300 ℃ salt bath cooling for a period of time and then air-cooled), in order to reduce the quenching stress, to prevent deformation and cracking.

3.Tempering

purpose: to eliminate quenching stress, adjust the hardness and toughness, stable organization and size.
Process parameters:
low-temperature tempering: 150-250 ℃, insulation 2-3 hours, air-cooled, tempered hardness of 58-62HRC, for molds requiring high hardness and wear resistance.
Medium temperature tempering: 300-500 ℃, insulation 2-3 hours, air-cooled, tempered hardness of 50-58HRC, can improve the toughness, suitable for molds subject to impact load.
High-temperature tempering: 500 ℃ or more, insulation 2-3 hours, air-cooled, tempered hardness 45-50HRC, mainly for the need for higher toughness of the occasion.

4. Precautions

heating process should control the rate of heating to avoid too rapid a rise in temperature leading to workpiece surface oxidation and decarburization. Protective atmosphere heating can be used or placed in the furnace charcoal and other anti-decarburization agent.
When quenching and cooling, choose the appropriate cooling medium and cooling method according to the shape and size of the workpiece to ensure the quenching effect while reducing the risk of deformation and cracking.
Tempering must be sufficient to ensure the elimination of internal stresses to avoid mold failure due to stress release during use. For large molds or workpieces with complex shapes, multiple tempering can be used.

1.2316 Tool Steel Quality Inspection

1. Surface condition inspection

Surface condition inspection

FCS factory has a very strict quality inspection team, we will carefully check the surface condition of each 1.2316 STEEL round steel and plate, to ensure that the surface of the steel is free from defects such as cracks, folding, scars, oxidized skin, pitting, scratches and so on.

2. Chemical Composition Testing

Chemical detection

To verify that the content of alloying elements meets the standard requirements and to safeguard the basis of the mechanical properties of the material. We will let the staff use full-spectrum direct reading spectrometer to analyze multiple elements at the same time. Sampling needs to remove the surface oxidation layer, using a block specimen to stimulate the test.

3.Dimension and Tolerance Inspection

Dimension and tolerance inspection

FCS factory will use professional measuring tools to inspect the dimensions and tolerances of the steel to ensure compliance with the customer's contract requirements. Corresponding gauges will be selected according to the dimensional accuracy requirements, including tape measure, high-precision vernier calipers (0.02mm), micrometers (0.001mm), and special inspection gauges. Inspection items cover: diameter, thickness, width, length, hole diameter, chamfering dimensions, etc., to ensure that the tolerances and dimensions meet the contract requirements.

4.Hardness test

Hardness testing

Our FCS factory will use a professional hardness tester to test the hardness of steel to ensure that it meets the customer's contract requirements.

5.Ultrasonic Testing

Ultrasonic detection

Ultrasonic Testing Standard (UT Test Standard) is: Sep 1921-84 Class3 D/d,E/e.
FCS factory uses ultrasonic testing equipment to detect macro defects inside the material (such as cracks, shrinkage holes, inclusions, white spots, etc.), and every piece of round steel and plate will be examined by a second flaw detection test before shipment to ensure that the quality is qualified before shipment.

6.Microstructure Inspection

Metallographic micro

(1) Metallographic Analysis

FCS factory will use metallographic analysis instrument to inspect the microstructure state after heat treatment, including carbide distribution, martensite morphology, residual austenite content, etc.

(2)Grain size rating

FCS factory will use the comparative method to determine the austenite grain size by comparing the microstructure of the specimen with the standard rating chart, to ensure that it meets the customer's requirements.

1.2316 Technical Specifications

Property Specification Standard/Method
Material Designation 1.2316 / X36CrMo17 DIN / EN
Default Supply Hardness 280-320 HB (28-34 HRC) ISO 6508
Density 7.7 g/cm³ ASTM B311
Thermal Conductivity 20 W/m·K (at 20°C) ASTM E1461
Specific Heat 460 J/kg·K ASTM E1269
Coefficient of Thermal Expansion 11.0×10⁻⁶/K (20-200°C) ASTM E228
Young's Modulus 215,000 N/mm² ASTM E111
Electrical Resistivity 0.65 Ω·mm²/m ASTM B193
Corrosion Resistance Excellent against organic acids, moderate against inorganic acids ASTM B117
Polishability Excellent (Ra < 0.01 μm achievable) ISO 4287

1.2316 Tool Steel Product Applications

Key Application Scenarios

Highly corrosive plastic molds

  1. Injection molds (PVC, recycled materials, fluorine-containing plastics);
  2. Extrusion molds (plastic pipes, chemical containers).

Precision tools

  1. Die casting molds, cold extrusion molds, mirror polishing molds;
  2. Food processing equipment parts (need to be corrosion-resistant and hygienic standards).

Mechanical parts

  1. Water pump shafts, compressor parts, high stress shear tools

1.2316 Tool Steel Competitive Advantage Table

Characteristics FCS'S1.2316 Tool Steel Standard Stainless Tool Steels P20 Tool Steel
Corrosion Resistance Excellent against organic acids and PVC gases Good only for atmospheric conditions Poor, requires coating
Polishability Excellent Good Very good
Machinability in Supply Condition Good (40-45% relative to C45) Poor to moderate (30-35%) Very good (45-50%)
Dimensional Stability Excellent (<0.05% change) Moderate (0.08-0.12% change) Good (0.05-0.08% change)
Weldability Good with proper procedures Poor to moderate Good with proper procedures
Temperature Resistance Good up to 400°C Excellent up to 550°C Moderate up to 350°C
Cost-effectiveness for PVC Processing High (extended tool life) Moderate (high initial cost) Low (frequent replacement)
1.2316 Tool Steel Customer Success Stories
Skip the middleman link, source factory purchasing, reduce purchasing cost and improve market competitiveness.

1.2316 Tool Steel Pricing Structure Information

Serving the world, whole cabinet sales, factory wholesale price.

1.2316 Tool Steel Frequently Asked Questions

Q: How does 1.2316 differ from standard stainless steel?
A. 1.2316 has excellent corrosion resistance to organic acids while maintaining excellent mechanical properties and machinability. Unlike standard stainless steels, it is pre-hardened and achieves a mirror-polished quality.
Q: How does 1.2316 compare to 420 stainless steel?
A: 1.2316 has similar corrosion resistance, but has superior mechanical properties, better polishability, and is prehardened. It exhibits better dimensional stability during heat treatment and better machinability in the hardened state.

Reviews

There are no reviews yet.

Be the first to review “1.2316 Tool Steel”

Your email address will not be published. Required fields are marked *